Dr. Fritsch delivers 1000 field-assisted sintering presses

September 29, 2015

Dr. Fritsch, a manufacturer of field-assisted sintering systems based in Fellbach, Germany, has announced the delivery of its 1000th sinter press. The company stated that Oxford University, UK, received the new sinter press machine which is capable of sin ... Read more »

Recent issue of Powder Metallurgy review - your go-to resource to stay updated on the world of powder metallurgy and metal powders

Expansion at Atomising Systems

July 15, 2015

Atomising Systems Ltd, Sheffield, UK, has reported that it has expanded its workforce to cope with a major influx of orders for metal powder. Staff numbers at its Darnall facility have increased from 35 in September 2014 to over 60 in June 2015 to allow t ... Read more »

Recent issue of Powder Metallurgy review - your go-to resource to stay updated on the world of powder metallurgy and metal powders

Hart Materials moves to new technology centre

July 28, 2014

After almost 10 years of operating from Carrier’s Fold Wombourne, South Staffordshire, UK, raw materials and metal powder supplier Hart Materials has moved to a newly refurbished Technology Centre in the same locality. Managing Director Dr Tony Hart ... Read more »

Recent issue of Powder Metallurgy review - your go-to resource to stay updated on the world of powder metallurgy and metal powders

In the latest issue of PM Review…

PM Review Spring 2023

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • GKN Powder Metallurgy: A strategic vision for the future of permanent magnets for EVs
  • Building trust in the Powder Metallurgy industry: The role of standardisation and an update on recent work by ISO/TC 119
  • High-volume powder production for Additive Manufacturing: SMS group’s continuous metal powder production process
  • Development of enhanced-performance PM brake pads for high-speed trains by Beijing Tianyishangjia New Material Corp., Ltd.
  • The START project: Creating a sustainable supply chain for green energy harvesting products by Powder Metallurgy
  • World PM2022: Reviewing three innovative methods for metal powder production

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

From the industry…

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
Download PDF