DuPont develops new lower-cost process for titanium powder
October 9, 2007
DuPont Titanium Technologies, based in Wilmington, Delaware, said to be the world’s largest producer of titanium dioxide (TiO2) – a white pigment used widely in the coatings, plastics and paper industries, has developed a new process for making high-pur ... Read more »