The “PM-13 International Conference & Exhibition on PM for Automotive and Engineering Industries”, 7-9 February 2013, India, organised by the PMAI, included a special session entitled “Precision & Additive Manufacturing”. Professor Ramamohan Tallapragada presents an overview of the session exclusively for ipmd.net.

fig1

Fig. 1 Layers of UV sensitive liquid polymer are solidified

using a laser (Courtesy 3D Systems)

This special session began with a presentation from Prof K P Karunakaran, Mechanical Engineering Department, IIT Bombay, who traced the beginnings of Additive Manufacturing (AM) back to 1987, when 3D Systems launched Stereo-Lithography Apparatus (SLA) and demonstrated a new way of manufacturing through addition. New processes known as Rapid Prototyping (RP) or 3D Printing or, more appropriately, Layered Manufacturing (LM) came into vogue.

The production of effective tools via this process resulted in a drastic reduction in ‘time-to-market’. The capabilities of RP expanded in terms of materials, quality and process capabilities, from initially only making polymer components to now being capable of producing ceramic and metallic parts.

Several post-build processes have emerged today to improve the surface quality (e.g. liquid polishing) and material integrity (for example, Hot Isostatic Pressing (HIP)). RP& AM, in conjunction with these post-build processes, allows rapid development of even very complex products such as those used in an aero engine. 

fig2

Fig. 2 LOM bonds and cuts sheet material using a computer guided laser (Courtesy Helisys)

Prof Karunakaran identified some of the unique capabilities of RP & AM as allowing:

  • Components/tools with conformal cooling channels,
  • Objects with gradient materials,
  • Components of non-equilibrium materials,
  • Assemblies without joints (elimination of welded joints),
  • Difficult/impossible shapes by other means
  • Customised solutions for aesthetic, ergonomic and bio-medical applications.

It was suggested that the term “3D printing” refers to economical AM processes, in the range of  USD $5,000-25,000, which can be part of any design office just as with 2D printers. This equipment is only suited to the quick physical realisation of a design for visualisation and review. Rapid Prototyping (RP) is a more advanced form of this process, which caters to mostly polymer components, but with assured quality and wide variety of materials so that they can be used for more complex applications of form, fit and functional tests. Rapid Manufacture (RM) is seen as the highest level which includes metals and ceramics and goes beyond prototyping. RM, through its many facets of direct and indirect routes (Vacuum Casting, Epoxy Tooling, Rapid Casting etc.), can be useful in regular production as well. While 3D printing and RP have linearity of cost with quantity, RM has the distinction of cost reducing with quantity.

fig3

Fig. 3 Cost comparisons for production of components via Additive Manufacturing (Courtesy Höganäs)

Deepak Grover and Hans Söderhjelm, Höganäs Digital Metal, described Additive Manufacturing as a process of building components in layers directly from 3D CAD data, without the need for complex and expensive tools and with minimal waste material. Unlike Rapid Prototyping, Additive Manufacturing goes to the next level by being able to mass produce end user products.

fig4

Fig.4 Digital Metal was used to manufacture the

‘Klein Bottle Opener’  (Courtesy Höganäs)

Höganäs Digital Metal, stated Grover, offers a revolutionary and innovative manufacturing technique for metallic components. It is a proprietary precision ink-jet technology for Additive Manufacturing and 3D printing of metal components and systems. This offers a unique capacity to rapidly and cost effectively produce highly complex and intricate designs and features for metallic parts.

Dr Mukesh Agarwal, 3D Product Development (3DPD), Bangalore, felt that today’s product development requirements have become more demanding, with the gap between product design cycle and mass manufacturing often required to be bridged by low volume production quantities. The product life cycles became shorter and, in many cases, products are being designed for limited volume.

This demand for low volume production has resulted in conventional Rapid Prototyping processes being adapted and adopted as “Additive Manufacturing” for low volume production. According to Dr Agarwal, given material limitations with traditional Rapid Prototyping processes, these processes are sometimes not even suitable to produce fully functional prototypes.

Powders and feedstock

Dr Rama Mohan R Tallapragada, Consultant, Mumbai, India, discussed the importance of powders and feedstock for successful Additive Manufacturing. During his presentation he referred to his paper presented during PM-02, the 2nd International conference on Powder Metallurgy in Automotive Applications held at New Delhi in 2002. That paper dealt with the then emerging techniques of Rapid Prototyping and their usefulness. A decade later his presentation discussed the rapid changes in the technologies such as production of prototypes, visual design aids, touch, feel, fit and assembly test parts, etc., that are used in the product development phase. For the real production parts at all levels the technology had evolved into Rapid Manufacturing techniques. These generally refer to techniques, he stated, that produce shaped parts by gradual creation or addition of material, as distinguished from forming and manufacturing through material removal.

The need for production of complex components with little or no machining by Powder Metallurgy (PM) techniques has seen injection moulding become a popular processing technique. The tools and dies required for injection moulding are themselves complex and in order to process these, the technology of Rapid Prototyping or Solid Free-form Fabrication (SFF) etc. has been utilised.

A Computer Aided Design (CAD) model of the required free-form is created and converted into STL format (after the process Stereo Lithography, for which 3D systems developed this format). The latter is sliced into thin cross-sectional layers and the output is fed to the Rapid Prototyping machine which then builds the free-form, one layer at a time. The free-form is then sintered to yield the final product.

Many layered manufacturing techniques are in vogue, with the most popular being: photo-polymerization (Stereo lithography (SLA) and its derivates), ink-jet printing (IJP), 3D printing (3DP), Fused Deposition Modeling (FDM), Selective Laser Sintering or Melting (SLS/ SLM and EBM1) and to a lesser extent Laminated Object Manufacturing (LOM and similar sheet stacking processes) and laser cladding (LC) processes. Many of the techniques are, however, limited to Rapid Prototyping as they do not allow common engineering materials to be processed with sufficient mechanical properties.

fig5


Fig. 5 FDM extrudes thermoplastic materials in filament form to produce parts layer by layer (Courtesy Stratasys)

The RM techniques are extensively used in processing ceramics and ceramic-polymer composites. The most popular techniques for metal powders are FDM and SLS. The latter often uses metal powders along with polymers. Complex shapes such as gears, turbine blades, etc. are produced.  

fig_3_laser

Fig. 6 Production of structured spheres by selective laser sintering (courtesy FIT)

Powders for laser sintering are generally spherical, fine and gas atomised. Where non spherical powders are to be used these should be coated with a polymeric binder and mixed to form loose agglomerates and then coated with lubricant/ plasticiser to minimise frictional forces and cause easy sliding.

In conventional sintering the particles are not fundamentally changed unlike in laser sintering, where the particles are fully or partially melted. Necessary feedstock properties include being free flowing with a size that must allow a reasonable finish. The binder must melt and “backbone” the powder to deliver required properties. Powder flow is affected by particle shape and size distribution, but the finer the powder the less it flows – the best combination is <50m and rounded.

The technology, however, is in the early stages as far as Powder Metallurgy applications are concerned. Developing a proper powder mix is a considerable challenge to the powder producers as it involves new generation inks, gels, pastes and powder blends etc. Some of the feed stock can be in the form of metal powder-polymer blends, wires, rods, granules etc. 

 

March 27, 2013

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Phoenix Sintered Metals: A story of transformation, growth and community from America’s PM heartland
  • World PM2024 Yokohama: The stage is set for the PM industry to find a path to sustainable growth
  • The state of Europe’s hard magnets industry and the challenge of optimising the mass production of Nd2Fe14B permanent magnets

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link