Foerster offers new induction thermography part testing

January 11, 2022

Comparison of a pinion in infrared (left) and with induction thermography (right), where a crack is visible in the gear root (Courtesy Foerster Group)

Foerster Group, headquartered in Reutlingen, Germany, has introduced a new, non-destructive automatable solution for testing sintered components using induction thermography. The technique allows for contact-free crack detection on metal components, and is particularly suited to parts with complicated shapes where test areas can be difficult or impossible to access with eddy current probes.

The process is reported to identify open cracks, pores, heat treatment cracks, forging laps, welding defects, etc. It can be used on rough, uneven surfaces and surfaces coated with water or oil, with testing done in less than one second.

The induction thermography method is suitable for the examination of semi-finished products as well as complexly shaped components. A current induced into the workpiece generates localised hotspots at the defects in the material. These hotspots can be detected through their heat radiation with an infrared camera.

A typical system consists of an infrared camera and an inductor, with a generator for high-power pulses. The inductor is positioned such that a magnetic field pulse induces currents in the test area, heating the part by a few degrees Celsius. Simultaneously the camera is recording the area. The camera captures the heat radiation, which is emitted as infrared light, and creates a temperature image of the surface.

Creases on the parts are particularly prone to crack. Such defects are accessible with thermography. However, very deep creases may also pose a challenge for this method (Courtesy Foerster Group)

If there are defects (cracks) in the test area, the induced current is deviated and is locally displaced or squeezed. Consequently, those locations in the part are heated stronger. When such hotspots form directly at the surface, they emit heat radiation and are visible to the camera. The heat from hotspots within the material can also reach the surface through the heat conduction of the material. However, the range into the material is limited by the penetration depth of the induction.

The thermal recordings are analysed with video and image processing algorithms. On a thermography recording, the hotspots leave a crack signature similar to a string of pearls. In contrast, other surface features, such as roughness and scratches, are suppressed. This way cracks can be detected that would be difficult or impossible to distinguish in a conventional photo. The high contrast and characteristic shape of cracks in induction thermography images allows for reliable algorithmic detection and enables the full automation of the procedure.

Induction thermography is said to offer a particular advantage on components that have special structural properties, such as threading, gearing, blades or profiles. Suitable parts include those that are forged, sintered and additively manufactured.

www.foerstergroup.com

Latest Industry News

Download the latest issue of PM Review

Our latest issue is now available to download in PDF format, free of charge.

As well as an extensive Powder Metallurgy industry news section, this 120-page issue includes the following exclusive articles and reports:

  • Tesla teardown: Identifying potential uses for PM in electric vehicle transmissions
  • Can European research still claim to be ‘world class’? Prof José M Torralba on the changed PM research base
  • How to make metal powders. Part 1: An introduction to atomisation, process fundamentals and powder characteristics
  • Starting out in powder production: The story of Fomas Group’s Mimete metal powder business
  • The creation of a Powder Metallurgy market leader: China’s NBTM New Materials Group Co., Ltd.
  • Tungsten heavy alloys: An exploration of how key property combinations enable better mechanical performance
  • Pharmaceuticals and PM are closer than you think: A new approach to understanding powder compaction and tablet characterisation
  • More information

Industry News

E-newsletter

Sign up to our free e-newsletter, sent weekly to industry professionals around the world. We'll also let you know each time a new issue of PM Review magazine is available.

Subscribe for a FREE digital magazine

PM Review is the leading international magazine for the Powder Metallurgy industry.
Published four times a year, it is available as a free download or through a print subscription

Connect with us

Powder Metallurgy: The original net-shape production process

Powder Metallurgy components are relied upon by a wide variety of manufacturing industries, from automotive to power tools, household appliances, chemical engineering, filtration and more.

The main reason for the technology’s success is its cost-effectiveness at producing high volumes of net-shape components, combined with its ability to allow the manufacture of products that, because of the production processes, simply cannot be manufactured by other methods.

To discover more about how the technology has revolutionised component production, browse our Introduction to Powder Metallurgy.

Latest industry news

Copy link