MPIF 2021 Powder Metallurgy Design Excellence Award winners
The winners in the 2021 Powder Metallurgy Design Excellence Awards competition, sponsored by the Metal Powder Industries Federation (MPIF), were announced during the International Conference on Powder Metallurgy and Particulate Materials (PowderMet2021), held in Orlando, Florida, USA, from June 20–23, 2021.
This year’s winners showcase PM’s diversity, with components used in a range of applications, from electric vehicles to ceiling fans. Designers use PM’s flexibility to push forward new concepts and process controls to demonstrate the capabilities PM can bring to critical applications such as auto engines and transmissions, medical devices, consumer products, hardware, and more.
In the design competition, a total of six Grand Prizes and sixteen Awards of Distinction were presented across the manufacturing categories of conventional Powder Metallurgy (PM), Metal Injection Moulding (MIM) and metal Additive Manufacturing.
Here, we highlight the Powder Metallurgy winners.
Grand Prizes
Automotive – Chassis Category PM
A Grand Prize in the Automotive – Chassis Category for Conventional PM components was awarded to Phoenix Sintered Metals LLC, USA, and its customer Dana Incorporated, for a stepped planetary gear used in a ridged rear axle gear box for battery electric light commercial vehicles. The five-level pinion is made using FL-4405-100HT.
It was essential to be able to deliver tight dimensional control for this complex shaped part, with the MPIF stating that no other metal forming technology could provide the part geometry at a commercially competitive price.
Hardware/Appliances Category PM
In the Hardware/Appliances Category for Conventional PM components, a Grand Prize was awarded to Metalpo Ind e Com Ltda and their customer Groupe SEB – Arno Clock Krups Panex Penedo Rochedo, for a soft magnetic composite (SMC) superior and inferior stator for a mono-phase induction motor for a ceiling fan. The component was specifically designed for the PM process to take advantage of the 3D magnetic flux, resulting in less copper wiring, a 76% reduction in the mass of the motor, and 35% less energy consumption and quieter operation.
Awards of distinction
Lawn & Garden/Off-Highway PM
In the Lawn & Garden/Off-Highway Conventional PM components Category, an Award of Distinction was presented to Sintergy Inc. and their customer Knott Brake Company for a drum brake shoe for off-highway units. The parts have localised infiltration to improve the region subject to wear. The PM parts replaced a three-piece weldment and passed extensive durability and performance testing.
In the Lawn & Garden/Off-Highway Conventional PM components Category, an Award of Distinction was also given to Singhal Sintered Pvt. Ltd. for bush speed gears for tractor transmissions. The previously forged parts have an inner diameter spline with a step. Maintaining the tight spline tolerance during the heat-treatment process was challenging. Finishing operations include OD grinding and face grinding.
Hand Tools/Recreation Category PM
In the Hand Tools/Recreation Category for Conventional PM components, an Award of Distinction has been given to Nichols Portland LLC for a positive displacement gerotor assembly for customised performance-racing fuel pumps. Racing applications require higher delivery pressures with fuel formulations that provide very low levels of lubricity. A novel material was developed to meet these needs in which a wear-resistant hard phase is dispersed within a matrix.
Industrial Motors/Controls & Hydraulics Category PM
In the Industrial Motors/Controls & Hydraulics Category for Conventional PM components, an Award of Distinction was given to Capstan for a coupling handle used to prevent accidental disconnects. Previously a casting, the conversion to PM permitted the elimination of the casting gate, incorporation of a locational pin-button hole and lettering. The coupling handles are used to provide improved pressure and temperature control capabilities in fluid power controls for a wide variety of applications.
Metal AM award winners
This year, the winners in the 2021 Powder Metallurgy Design Excellence Awards competition included three components made using metal Additive Manufacturing. Organised by the Metal Powder Industries Federation (MPIF), the awards were announced during the International Conference on Powder Metallurgy and Particulate Materials (PowderMet2021), an event co-located with the Additive Manufacturing with Powder Metallurgy (AMPM2021) and Tungsten2021 conferences, held in Orlando, Florida, USA, from June 20–23, 2021.
In the design competition, a total of six Grand Prizes and sixteen Awards of Distinction are presented across the manufacturing categories of conventional Powder Metallurgy (PM), Metal Injection Moulding (MIM) and metal Additive Manufacturing.
A Grand Prize was awarded to Parmatech Corporation, California, USA, in the Hand Tools/Recreation Category for Metal AM components for a 316L stainless steel putter head and hosel, made for Cobra Puma Golf, and used in the King Supersport-35 golf putter. The MPIF explained that the use of Additive Manufacturing technology has allowed designers to place or remove material strategically, ensuring the optimal mass distribution and stiffness. This flexibility also allowed the production of both right and left-hand versions of the putter head and hosel without the need for tooling changes. The development of unique lattice structures also eliminated the need for supports during the sintering process.
In the Aerospace/Military/Firearms Category for Metal AM components, 3DEO Inc., California, USA, received an Award of Distinction for a 17-4 PH stainless steel casing extractor for Glock brand pistols. A hybrid AM approach was said to have been used to make the part, offering the robustness and accuracy of CNC machining and the scalability of MIM, while overcoming the drawbacks of each process. The part has a complex geometry with several small, critical features.
3DEO Inc. received a further Award of Distinction in the Hand Tools/Recreation Category for an open comb base plate used in a double-edge safety razor for their customer Blackland Razors. A hybrid AM approach was also used to make the parts, offering tight dimensional tolerances that set the blade gap for this shaving razor.
Metal Injection Moulding award winners
The winners in the 2021 Powder Metallurgy Design Excellence Awards competition, sponsored by the Metal Powder Industries Federation (MPIF), were announced during the International Conference on Powder Metallurgy and Particulate Materials (PowderMet2021), held in Orlando, Florida, USA, from June 20–23, 2021.
In the design competition, a total of six Grand Prizes and sixteen Awards of Distinction were presented across the manufacturing categories of conventional Powder Metallurgy (PM), Metal Injection Moulding (MIM) and metal Additive Manufacturing.
This year, the awards were dominated by winners in the MIM category, receiving a total of thirteen awards and highlighting the continuing innovation seen in this sector. The winning parts are used in a wide range of applications, from firearms to electronic devices, and showcase the versatility MIM can bring to component design.
Here, we highlight the Metal Injection Moulding winners.
Grand Prizes
Aerospace/Military/Firearms Category MIM
In the Aerospace/Military/Firearms Category for MIM components, a Grand Prize was awarded to ARC Group Worldwide for an enclosed striker used in the firing mechanism of a commercial handgun. The position of the tip to the primary body of the component is said to be critical for part functionality.
The part is made in a two-cavity mould, with strategic tool design and staging being implemented. Post-sintering, HIP and heat treatments were performed to increase mechanical properties, and the parts are finished with an E-nickel coating.
Hand Tools/Recreation Category MIM
A Grand Prize was also awarded to ARC Group Worldwide in the Hand Tools/Recreation Category for MIM components, for a quick-disconnect assembly used for a variety of small handheld devices such as binoculars, cameras, and firearms. Utilising MIM allowed for a near-net-shape moulded assembly and enabled the incorporation of smooth transitions and rounded edges, as well as the elimination of any machining marks on the visible portions of the parts.
Medical/Dental Category MIM
In the Medical/Dental Category for MIM components, a Grand Prize was given to OptiMIM for a compression frame used in Nextremity Solutions Lapidus System for holding and aligning the targeting drill guide during tarsometatarsal fusion.
The parts are produced using MIM-420 stainless steel in a single cavity open and shut mould with two slides. The first forms the rectangular opening and the second the two holes at a 60º angle on the opposite end of the frame. The parts are sized in a die with two slides so that forces can be applied in perpendicular directions to the parts.
Awards of distinction
Automotive – Transmission Category MIM
In the Automotive – Transmission Category for MIM components, an Award of Distinction was given to ARC Group Worldwide for a worm gear used in a transmission locking mechanism. MIM processing was selected because of the complexity of the helical gear teeth and the adjacent shaft geometry. Custom staging furniture is used for sintering the parts which require no secondary operations to be functional in the mating assembly.
In the Automotive – Transmission Category for MIM components, an Award of Distinction was also presented to Indo-MIM Pvt. Ltd. for an oil spray piston cooler. The MIM-4605 parts are used in the engine of heavy vehicles and were previously made by machining. Holes are formed by two different slide pins at different angles in the tool, and the side core has to travel through the center pin with a delay mechanism.
Aerospace/Military/Firearms Category MIM
In the Aerospace/Military/Firearms Category for MIM components, an Award of Distinction was given to Indo-MIM Pvt. Ltd. for a frame chassis, part of a pistol assembly. The parts are made using MIM-17-4 PH in the H900 condition.
Prior to MIM the parts were machined from bar stock by the customer. The MIM parts meet 80% of the required part features with the remainder being machined by the customer, reducing the machining cycle by 70%.
In the Aerospace/Military/Firearms Category for MIM components, an Award of Distinction was also given to Advanced Powder Products Inc. and its customer Savage Arms for a bolt handle for a hunting rifle. The part assists with loading the next round of ammunition and in removing the shell after it has been fired.
The complex curvature and intricate design presented challenges with moulding and sintering. MIM processing was able to convert a two-piece design machined from bar stock to a single piece MIM part.
Industrial Motors/Controls & Hydraulics Category MIM
An Award of Distinction was given to Indo-MIM Pvt. Ltd. in the Industrial Motors/Controls & Hydraulics Category for MIM components for a casing and ground used in industrial gas sensors. Both parts require high magnetic permeability and low coercive field strength. The ground has many holes and threads, and the casing is a complex part with thin walls, sectional differences, and three threaded holes on the outer walls.
Hardware/Appliances Category MIM
In the Hardware/Appliances Category for MIM components, an Award of Distinction was awarded to Indo-MIM Pvt. Ltd. for a knob shaft, clutch, knob shield, core plug, core body, and control sleeve actuator used in door locks. The previously machined stainless-steel parts have intricate profiles, thin walls, multiple holes, blind threads, aesthetic requirements, and sectional differences adding to the complexity of the part.
In the Hardware/Appliances Category for MIM components, an Award of Distinction was also presented to ARC Group Worldwide for a key blade used in an electronic security system. Sintering requires custom staging to minimise distortion of the delicate geometries critical to part functionality. The parts require two sizing steps to ensure twelve critical dimensions meet the customer specifications. Fitment to the mating part and the aesthetic appearance of the primary visual surface was essential.
Medical/Dental Category for MIM
In the Medical/Dental Category for MIM components, an Award of Distinction was given to ARC Group Worldwide for a pusher used in the ratcheting assembly for the consistent placement of high viscosity adhesives in incisions, used as an alternative to sutures or staples in surgical procedures. Strategic tool design, venting and a three-plate pin gate allow complete material fill of the complex part geometry, keeping distortion to a minimum and allowing tight profile and dimensional requirements to be maintained.
An Award of Distinction has also been awarded in the Medical/Dental Category for MIM components to Alpha Precision Group – Metal Injection Molding and its customer Elite Biomedical Solutions for an LVP door latch for an IV pump. The component has a tight tolerance on the hole position for the assembled roller. In use, the roller is latched on to a mating component that the company also makes to complete the latch/hook mechanism. The parts are made in-house from start to finish and the machining and multi-stage assembly are considered value added to the customer.
Electronics/Electrical Components category MIM
In the Electronics/Electrical Components category for MIM components an Award of Distinction was awarded to Indo-MIM Pvt. Ltd. for a ceramic sensor used in an electronic device. Previously machined, the complex, mostly hollow parts have a U-shaped geometry with an open slot at the rear end and a through-hole at the front, with another hole passing horizontally through the slot.