Tekna secures $1.5 million order for titanium powder used in medical applications

ApplicationsMaterialsNews
November 27, 2023

November 27, 2023

Tekna Holding ASA, based in Sherbrooke, Quebec, Canada, has announced an order worth CA $1.5 million for titanium alloy powder used exclusively in medical applications. The contract represents a 60% increase in orders from this particular customer, compared to the previous year, and is part of a three-year distribution agreement.

The unnamed customer is reported to be a leading titanium powder distributor in the global medical and dental industry. Delivery is scheduled within the first three quarters of 2024.

THE WORLD OF POWDER METALLURGY TO YOUR INBOX
Subscribe to our weekly newsletter
Sign up

“This substantial order is a testament to Tekna’s growing influence and reputation in the advanced materials industry, particularly in the medical sector, which has grown to become one of the most advanced and prominent users of additive manufacturing on a global scale. Partnering with a key player in the European market not only strengthens our position but also highlights the trust and reliability associated with our products. We are proud to play a pivotal role in advancing medical technologies through our specialised titanium powders,” stated Luc Dionne, CEO of Tekna.

www.tekna.com

Download PM Review magazine
ApplicationsMaterialsNews
November 27, 2023

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Phoenix Sintered Metals: A story of transformation, growth and community from America’s PM heartland
  • World PM2024 Yokohama: The stage is set for the PM industry to find a path to sustainable growth
  • The state of Europe’s hard magnets industry and the challenge of optimising the mass production of Nd2Fe14B permanent magnets

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link