Swansea University brings small-batch metal powder production in-house with ATO Lab+

EquipmentMaterialsNews
February 14, 2024

February 14, 2024

The ATO Lab+ ultrasonic metal atomiser supplied by Analytik has enabled the Swansea team to swiftly produce small batches of novel alloy powders (Courtesy Analytik/Swansea University)
The ATO Lab+ ultrasonic metal atomiser supplied by Analytik has enabled the Swansea team to swiftly produce small batches of novel alloy powders (Courtesy Analytik/Swansea University)

Analytik, a supplier of scientific instruments for a range of applications, based in Cambridge, UK, has reported how Swansea University, Wales, has used an ATO Lab+ atomiser developed by 3D Lab, Warsaw, Poland, to support the university’s work in metal powder production for Additive Manufacturing applications.

Before integrating ATO Lab+ into its alloy development workflow, the Swansea University team faced significant hurdles, stated Analytik. The previous method of developing alloys for Additive Manufacturing involved using external suppliers to gas atomise the powder. This caused delays of approximately fourteen weeks and required a minimum batch size of 200 kg, leading to unnecessary waste. It meant that the team was unable to link its small-scale rapid alloy prototyping and in-house AM capabilities without external powder production.

THE WORLD OF POWDER METALLURGY TO YOUR INBOX
Subscribe to our weekly newsletter
Sign up

The ATO Lab+ ultrasonic metal atomiser supplied by Analytik has enabled the Swansea team to swiftly produce small batches of novel alloy powders, for faster, more efficient production within the university’s own lab. This speeds up alloy discovery for a wide range of cutting-edge applications.

Professor Nick Lavery, Director of the Materials Advanced Characterisation Centre (MACH1), and the lead academic of the Swansea Additive Manufacturing Research (SAMR) group, stated, “The ATO Lab+ machine is well manufactured and 3D Lab have been very helpful with all aspects including procurement, installation, commissioning, training and troubleshooting.”

Going forward, Swansea University plans to develop novel alloys for various Additive Manufacturing techniques, including Laser Beam Powder Bed Fusion (PBF-LB), Binder Jetting (BJT), blown powder, and Hot Isostatic Pressing (HIP).

www.metalatomizer.com

www.swansea.ac.uk

analytik.co.uk

EquipmentMaterialsNews
February 14, 2024

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Powder Metallurgy: Discover innovative technologies meeting the demands of vehicle electrification
  • Gevorkyan a.s.: Europe’s fast-growing Powder Metallurgy company achieving success through a diversified customer base
  • Powder Metallurgy in Asia: A status update from the World PM2024 Congress, Yokohama

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link