Retsch launches updated system for particle size and shape analysis

March 17, 2015

Retsch Technology GmbH, Haan, Germany, has launched the fourth generation of its Camsizer system for particle size and particle shape analysis. The Camsizer P4 features include an extended measurement range from 20 µm to 30 mm, faster cameras with higher resolution as well as a particle library for direct storage of individual particle images.  

camsizer

The Camsizer P4 is a compact laboratory instrument for simultaneous measurement of particle size distribution, particle shape and additional parameters of powders and granules. The system utilises dynamic image analysis through patented dual-camera technology.

The extended software functionalities now include an image library containing pictures and contours of each particle and its respective shape and size readings and a 3-dimensional diagram (3D Cloud scatterplot) of the analysis parameters. New particle shape descriptors allow for analysis of the roundness of particles.

The patented dual camera technology used by the Camsizer P4 and animations of the measurement procedure of dynamic image analysis can be seen in a new video. This not only explains the measurement technique and software features, such as the display of measurement results as 3D scatter plots, but also shows a variety of application areas as well as optional usage with an Autosampler and a process-line version.

www.retsch.com/camsizerp4  

See video here


Powder Metallurgy Review magazine:

Your email address:


Useful links: Download PM Review magazine | News headlines | Browse articles 



Powder Metallurgy Review magazine cover

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Hot Isostatic Pressing for the production of large, near-net shape components
  • Safeguarding PM part usage in a new automotive industry
  • How to make metal powders., Part 3
  • Company profile: Jiangxi Yuean Advanced Materials

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

From the industry…

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
Download PDF
Share via
Copy link