Höganäs adds 17-4 stainless steel to its Additive Manufacturing range

News
April 12, 2016

April 12, 2016

Sweden’s Höganäs AB has extended the range of materials suited to its Digital Metal® Additive Manufacturing technology by including high performance 17-4 PH stainless steel. According to Höganäs, 17-4 PH enables production of components with high strength and hardness.

The material is a hardening grade exhibiting considerably higher strength compared to the more commonly used austenitic 316L. It also provides improved corrosion resistance compared to 400 series ferritic stainless steels.

Digital Metal is a 3D metal printing technology enabling production of small and complex objects that would be costly, if not impossible, to produce using traditional methods.

www.hoganas.com  

News
April 12, 2016

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Phoenix Sintered Metals: A story of transformation, growth and community from America’s PM heartland
  • World PM2024 Yokohama: The stage is set for the PM industry to find a path to sustainable growth
  • The state of Europe’s hard magnets industry and the challenge of optimising the mass production of Nd2Fe14B permanent magnets

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link