Hoeganaes to form new joint venture to produce titanium powder in North America

July 27, 2016

Hoeganaes to form new joint venture to produce titanium powder

Photomicrograph of AncorTiTM Titanium Powder

GKN Hoeganaes has agreed to enter into a joint venture agreement with TLS Technik to manufacture titanium powders in North America for Additive Manufacturing applications. It was stated that the new facility is planned to open in 2017.

TLS is located in Bitterfeld, Germany and has 20 years of experience manufacturing titanium powder for the AM market. The new joint venture complements GKN’s previously announced powder R&D efforts in Cinnaminson, New Jersey and provides its customers with a North American source for titanium powders especially for the growing aerospace and medical markets.

GKN Hoeganaes, a subsidiary of GKN Powder Metallurgy, is a producer of metal powders for structural components with metal powder manufacturing facilities in the United States, Europe and Asia.

www.hoeganaes.com

Powder Metallurgy Review magazine cover

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Hot Isostatic Pressing for the production of large, near-net shape components
  • Safeguarding PM part usage in a new automotive industry
  • How to make metal powders., Part 3
  • Company profile: Jiangxi Yuean Advanced Materials

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

From the industry…

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
Download PDF
Share via
Copy link