Gasbarre receives multiple batch steam treater orders

March 19, 2020

Gasbarre has received three separate orders for batch steam treaters (Courtesy Gasbarre Thermal Processing Systems)

Gasbarre Thermal Processing Systems, based in St. Marys, Pennsylvania, USA, part of Gasbarre Products Inc., has received three separate orders for batch steam treating equipment. Steam treating processes are used in many different industries and these orders will be shipped to companies that provide products to the medical, Additive Manufacturing, automotive and consumer products sectors.

The batch steam treaters produce an oxide layer that promotes corrosion and wear resistance properties and provides an attractive surface finish. The performance and quality of the surface and subsurface layers depends to a great extent on surface cleanliness and the overall (atmosphere) integrity of the equipment.

The three orders range in size from 45 cm to 76 cm diameter and 30 cm to 121 cm deep. The gross load weight capacity ranges from 136 kg to 816 kg with Gasbarre supplying the production tooling. The equipment is electrically heated and has a maximum operating temperature rating of 760℃.

www.gasbarre.com/thermal-processing-systems

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Phoenix Sintered Metals: A story of transformation, growth and community from America’s PM heartland
  • World PM2024 Yokohama: The stage is set for the PM industry to find a path to sustainable growth
  • The state of Europe’s hard magnets industry and the challenge of optimising the mass production of Nd2Fe14B permanent magnets

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link