AXT to bring Amazemet’s Additive Manufacturing tech to Australian market

June 21, 2023

Amazemet’s rePowder ultrasonic powder atomiser and alloy prototyping platform for batch production of spherical alloy powders (Courtesy Amazemet)
Amazemet’s rePowder ultrasonic powder atomiser and alloy prototyping platform for batch production of spherical alloy powders (Courtesy Amazemet)

AXT, a supplier of scientific equipment headquartered in Sydney, Australia, has announced that is has partnered with Amazemet Sp. Z o. o., based in Warsaw, Poland, to bring its range of Additive Manufacturing equipment to the Australian market.

“3D printing is an extremely dynamic sector and we are excited by the prospect of becoming more involved by partnering with Amazemet to assist Australian researchers and companies to accelerate their development projects,” stated Richard Trett, AXT’s Managing Director.

THE WORLD OF POWDER METALLURGY TO YOUR INBOX
Subscribe to our weekly newsletter
Sign up

Amazemet, a spin-off of the Warsaw University of Technology, designs and manufactures a range of systems for those involved in metal Additive Manufacturing, with products spanning from R&D to small-scale industrial production. The company has successfully transferred ultrasonic atomisation technology, along with expertise in automated support removal and post AM heat treatment, into devices that are now part of its portfolio.

“We are currently experiencing rapid growth with systems being installed all around the world,” added Łukasz Żrodowski, Amazemet CEO. “It made sense for us to look at the Australian market and we are proud to partner with AXT on this journey which I am sure will yield results in the short term.”

One of Amazemet’s leading systems is the rePowder, a fully customisable, modular designed system optimised to economically produce small quantities of highly spherical metal powders with narrow size distributions and free flowing characteristics, said to be perfect for metal Additive Manufacturing. Using ultrasonic atomisation, rePowder can reportedly produce powders from virtually any feedstock in a more cost-effective and efficient process compared to typical gas atomisation. This makes it ideal for R&D, where experiments with a specific powder compositions, or a small quantity of powder for a particular job, is required.

Amazemet’s other products include the safeEtch and inFurner. safeEtch is a system that uses a patented chemical solution to remove supports from metal parts quickly and easily. inFurner is a compact vacuum furnace suited to the post-heat treatment of metal AM parts, as well as the heat treatment of other materials requiring a controlled atmosphere.

www.amazemet.com

www.axt.com.au

Download PM Review magazine

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Phoenix Sintered Metals: A story of transformation, growth and community from America’s PM heartland
  • World PM2024 Yokohama: The stage is set for the PM industry to find a path to sustainable growth
  • The state of Europe’s hard magnets industry and the challenge of optimising the mass production of Nd2Fe14B permanent magnets

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link