Titanium foams replace injured bones

.resized_350x258_titanium_foam_IFAM

Flexible yet rigid like a human bone, and immediately capable of bearing loads: A new kind of implant, made of titanium foam, resembles the inside of a bone in terms of its structural configuration. Not only does this make it less stiff than conventional massive implants. It also promotes ingrowth into surrounding bones.

The greater one‘s responsibilities, the more a person grows. The same principle applies to the human bone: The greater the forces it bears, the thicker the tissue it develops. Those parts of the human skeleton subject to lesser strains tend to have lesser bone density. The force of stress stimulates the growth of the matrix. Medical professionals will soon be able to utilize this effect more efficiently, so that implants bond to their patients‘ bones on more sustained and stable basis. To do so, however, the bone replacement must be shaped in a manner that fosters ingrowth – featuring pores and channels into which blood vessels and bone cells can grow unimpeded. Among implants, the titanium alloy Ti6Al4V is the material of choice. It is durable, stable, resilient, and well tolerated by the body. But it is somewhat difficult to manufacture: titanium reacts with oxygen, nitrogen and carbon at high temperatures, for example. This makes it brittle and breakable. The range of production processes is equally limited.

There are still no established processes that can be used to produce complex internal structures. This is why massive titanium implants are primarily used for defects in load-bearing bones. Admittedly, many of these possess structured surfaces that provide bone cells with firm support. But the resulting bond remains delicate. Moreover, the traits of massive implants are different from those of the human skeleton: they are substantially stiffer, and, thus, carry higher loads. “The adjacent bone bears hardly any load any more, and even deteriorates in the worst case. Then the implant becomes loose and has to be replaced”, explains Dr.-Ing. Peter Quadbeck of the Fraunhofer Institute for Manufacturing and Advanced Materials IFAM in Dresden. Quadbeck coordinates the ‘TiFoam’ Project, which yielded a titanium-based substance for a new generation of implants. The foam-like structure of the substance resembles the spongiosa found inside the bone.

 

The titanium foam is the result of a powder metallurgy-based molding process that has already proven its value in the industrial production of ceramic filters for aluminum casting. Open-cell polyurethane (PU) foams are saturated with a solution consisting of a binding medium and a fine titanium powder. The powder cleaves to the cellular structures of the foams. The PU and binding agents are then vaporized. What remains is a semblance of the foam structures, which is ultimately sintered. “The mechanical properties of titanium foams made this way closely approach those of the human bone”, reports Quadbeck. “This applies foremost to the balance between extreme durability and minimal rigidity.” The former is an important precondition for its use on bones, which have to sustain the forces of both weight and motion. Bone-like rigidity allows for stress forces to be transmitted; with the new formation of bone cells, it also fosters healing of the implant. Consequently, stress can and should be applied to the implant immediately after insertion.

 

In the ‘TiFoam’ project, the research partners concentrated on demonstrating the viability of titanium foam for replacement of defective vertebral bodies. The foam is equally suitable for repairing other severely stressed bones. In addition to the materials scientists from the Fraunhofer institutes IFAM and IKTS – the Institute for Ceramic Technologies and Systems in Dresden – physicians from the medical center at the Technical University of Dresden and from several companies were involved in developing the titanium foam. Project partner InnoTERE already announced that it would soon develop and manufacture ‘TiFoam’-based bone implants.


For more information contact

Dr.-Ing. Peter Quadbeck

or Cornelia Müller

www.fraunhofer.de

 

Recent issue of Powder Metallurgy review - your go-to resource to stay updated on the world of powder metallurgy and metal powders

In the latest issue of PM Review…

PM Review Spring 2023

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • GKN Powder Metallurgy: A strategic vision for the future of permanent magnets for EVs
  • Building trust in the Powder Metallurgy industry: The role of standardisation and an update on recent work by ISO/TC 119
  • High-volume powder production for Additive Manufacturing: SMS group’s continuous metal powder production process
  • Development of enhanced-performance PM brake pads for high-speed trains by Beijing Tianyishangjia New Material Corp., Ltd.
  • The START project: Creating a sustainable supply chain for green energy harvesting products by Powder Metallurgy
  • World PM2022: Reviewing three innovative methods for metal powder production

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

From the industry…

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
Download PDF
Share via
Copy link