Vale’s Goro site produces its first nickel metal product

News
August 12, 2010

August 12, 2010

Vale (formerly Vale Inco) headquartered in Rio de Janeiro, Brazil, has announced that the Goro project has successfully produced its first nickel metal product.

Located in New Caledonia in the South Pacific, Vale confirmed that commissioning at the Goro plant is now almost complete. Remaining commissioning work will continue to take place over the next few months with the refinery expected to be in production by the end of this year.

Goro is a nickel laterite project with an estimated annual nominal capacity to produce 60,000 metric tons of nickel and 4,000 metric tons of cobalt as a by-product.

Nickel is widely used to produce stainless steel and special alloys. It is an essential ingredient in the products we use every day, including electronics, construction materials and medical equipment.

Vale has more than 12,000 employees working with nickel in Canada, the United States, Indonesia, Asia, New Caledonia, the United Kingdom and Brazil.

www.nickel.vale.com

News
August 12, 2010

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • From powder modification to rejuvenation: Fluidised Bed Reactors in metal powder production and Additive Manufacturing
  • Retech: Enabling the atomisation of reactive and refractory alloys at substantially higher levels of productivity and lower cost
  • Sustainability in Powder Metallurgy: Highlights from the 41st Hagen Symposium
  • Innovations from Japan’s Powder Metallurgy industry: award winners highlight novel automotive and healthcare applications

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link