Reading Alloys' senior R&D metallurgist gives talk on titanium powders for medical applications

Muktesh Paliwal, Senior R&D Metallurgist at Reading Alloys at the APMI West Penn presentation (Courtesy Ametek Specialty Metal Products)

 

Muktesh Paliwal, a Senior R&D Metallurgist at Reading Alloys, a division of Ametek Specialty Metal Products, Pennsylvania, USA, gave a keynote presentation on the topic of titanium powders for medical applications at a Technical Session of the West Pennsylvania Chapter of the American Powder Metallurgy Institute (APMI International), which took place in St. Mary’s, Pennsylvania, USA.

Paliwal presented an overview of Reading Alloys’ expertise in the field, including the processes involved in the production of titanium powders and alloys. He also explained the advantages that titanium powders and alloys offer the medical industry for specialist surgical, dental and cardiovascular applications.

In his talk, Paliwal cited Reading Alloys’ titanium powders for orthopaedic implants as an example of innovation in the medical industry. He went on to explain how spray coating can provide excellent surface conditions for hip joints, as it enables the bone to grow into the implant through a process known as osseointegration, which anchors the implant to provide longevity.

According to Reading Alloys, titanium is ideal for medical applications due to its high corrosion resistance. Other advantages include its low density and high specific strength, as well as its compatibility with MRI and CT technology. The company’s titanium powders include CP Ti, magnesium and sodium-reduced Ti sponge, Ti Hydride and Ti-6Al-4V.

Paliwal also described how Reading Alloys produces master alloys using thermite processes to create more than sixty standard alloy formulations, tailored according to customer specifications. These master alloys can be mixed with titanium sponge and melted to make various titanium alloys by customers.

“People are living to an older age now and have an increased desire to stay active for longer and maintain a good quality of life. As a consequence, demand has increased for critical medical applications, such as heart valves, hearing aids, hip implants, stents and other implantable devices. We are proud to see our specialist metal powder, tube and strip products – particularly our medical plasma spray coatings – becoming increasingly key in the evolution of devices like these,” stated Paliwal.

www.ametek.com

News
April 17, 2019

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • From powder modification to rejuvenation: Fluidised Bed Reactors in metal powder production and Additive Manufacturing
  • Retech: Enabling the atomisation of reactive and refractory alloys at substantially higher levels of productivity and lower cost
  • Sustainability in Powder Metallurgy: Highlights from the 41st Hagen Symposium
  • Innovations from Japan’s Powder Metallurgy industry: award winners highlight novel automotive and healthcare applications

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link