Ivor Jenkins Medal presented to Dr John Dunkley The UK’s Institute of Materials, Minerals and Mining (IOM3) has presented its 2016 Ivor Jenkins Medal to Dr John Dunkley CEng, FIMMM, Chairman of Atomising Systems Limited, UK. The prestigious award is presented to individuals in recognition of a significant contribution that has enhanced the scientific, industrial or technological understanding of materials processing or component production using Powder Metallurgy and particulate materials.

Dr Dunkley has over 40 year’s experience in atomising plant technology, dating back to his early career when he started the Davy-McKee operation that supplied and installed such plant in 1974. When Davy-McKee decided to withdraw from this business in 1992 he founded his own company, Atomising Systems Limited (ASL).

ASL has now built and supplied around 140 plants to customers in 34 countries. These range from major powder suppliers, of whom around half have dealt with ASL, to small in-house operations.

The company has developed many specialist powders, including water atomised stainless steel powders for filter applications, gas atomised Ag-28Cu powder for brazing and Gas atomised special Cu alloys for diamond tool manufacture. Significant atomisation technology developments made have included technology for the production of satellite-free powders in gas atomisation, ultrasonic vibratory atomisation used for very narrow size range, perfectly spherical solder powder production for electronics and centrifugal (spinning cup) atomisation – which is also used in the latest electronic solder powder plants.

Dr Dunkley also served for several years as Chair of the IOM3 Particulate Engineering Committee.

www.iom3.org

www.atomising.co.uk

News
July 13, 2016

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • From powder modification to rejuvenation: Fluidised Bed Reactors in metal powder production and Additive Manufacturing
  • Retech: Enabling the atomisation of reactive and refractory alloys at substantially higher levels of productivity and lower cost
  • Sustainability in Powder Metallurgy: Highlights from the 41st Hagen Symposium
  • Innovations from Japan’s Powder Metallurgy industry: award winners highlight novel automotive and healthcare applications

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link