EOS highlights new developments in laser sintered titanium orthopaedic implants

News
February 17, 2011

February 17, 2011

EOS Electro Optical Systems GmbH based in Krailling, Germany, displayed a new range of titanium based orthopaedic implants, manufactured by selective laser sintering, at this year’s American Academy of Orthopaedic Surgeons (AAOS) annual meeting in San Diego (15-19 February).

eos_1

Orthopedic implants laser-sintered in titanium

As well as the implants, parts exhibited included customised surgical drill guides reflecting patient-specific geometry, bone rasp samples, and prototype stainless steel surgical tools.

Martin Bullemer, EOS Manager for medical business development, stated, “Metal and plastics laser sintering have clearly become enabling technologies for medical products.”

eos_2

Implants manufactured in batches with direct

metal laser-sintering (DMLS)

EOS plastic and metal laser-sintering systems allow medical designers to tailor parts specifically for doctors and patients using 3D data generated by MRI, CT, and/or CAD. Modern data preparation software in combination with laser-sintering can be used to create complex geometries, porous surfaces suitable for better osteointegration or lightweight structures to promote better patient comfort.

 

www.eos.info  

 

Also available from Inovar Communications:

Titanium and titanium alloys for medical applications: opportunities and challenges

Titanium powder injection moulding (Ti-PIM): A review of the current status of materials, processing, properties and applications

 

News | Articles | Market reviews | Search directory | Subscribe to e-newsletter

 

www.ipmd.net

Published on www.ipmd.net

News, articles and a fully searchable directory for the powder metallurgy industry

News
February 17, 2011

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • From powder modification to rejuvenation: Fluidised Bed Reactors in metal powder production and Additive Manufacturing
  • Retech: Enabling the atomisation of reactive and refractory alloys at substantially higher levels of productivity and lower cost
  • Sustainability in Powder Metallurgy: Highlights from the 41st Hagen Symposium
  • Innovations from Japan’s Powder Metallurgy industry: award winners highlight novel automotive and healthcare applications

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link