VBN Components receives award for its cemented carbide Vibenite alloy

June 29, 2020

A Vibenite 480 compressor screw (Courtesy VBN Components)

VBN Components, Uppsala, Sweden, has received a “Best of Industry Award” in the category of Additive Manufacturing from Germany’s MM Maschinenmarkt, for its cemented carbide Vibenite® 480 alloy. The company received the award on June 25, during an online ceremony broadcast from Würzburg, Germany.

The company states that the patented Vibenite 480 alloy is extremely heat-resistant (up to at least 750°C) and wear-resistant and corrosion-resistant. Processing via Additive Manufacturing is enabling the production of complex shapes for industrial tools and components, and reducing environmental impact.

According to VBN Components, the Vibenite 480 is based on metal powder produced through large scale industrial gas atomisation, said to minimise both cost and environmental impact. The new material combines the toughness of Powder Metallurgy High-Speed steels (PM-HSS) with the heat resistance of cemented carbides, which is why this new group of materials is named as hybrid carbides.

Vibenite 480 has a carbide content of ~65% but is said to be tougher than regular cemented carbides and therefore suitable for more complex details. Typical applications for this material are cutting tools for milling, drilling and gear cutting, which require good wear resistance at high temperatures, combined with good toughness. The AM process opens up completely new possibilities in the design of the tools, states the company.

A ground “diamond” in Vibenite 480, showing a smooth and pore-free material (Courtesy VBN Components)

In addition, Vibenite 480 is also reportedly suitable for all components that are subject to high wear, such as pump components, nozzles, and baffle plates – said to be an ideal alternative to hard metals or wear-resistant alloys. 

Due to Additive Manufacturing, the components can rapidly be produced in near-net-shape, with design options offering new approaches to make components more wear-resistant. Additively manufactured cutting tools or wear components can be manufactured with very short lead times, which opens up many new approaches to build, test and improve prototypes and finally take the optimised component or cutting tool to serial production.

“Germany is a very important market for us, and we are delighted to receive this award in this heavy competition,” commented Ulrik Beste, CTO of VBN Components. “The company vision is to renew the materials industry in the world by developing materials that offer uniqueness and improved industrial performance, and the Best of Industry Award is a great recognition to our achievement.”

www.vbncomponents.se

Latest Industry News

Download the latest issue of PM Review

Our latest issue is now available to download in PDF format, free of charge.

As well as an extensive Powder Metallurgy industry news section, this 88-page issue includes the following exclusive articles and reports:

  • Are you safe or lucky? A look at Environment, Health and Safety in the PM industry
  • The hybridisation of pick-up trucks and the impact on the content of PM parts
  • EPMA’s General Assembly reviews Powder Metallurgy trends in Europe
  • Metal powder recycling: Innovative technology is turning waste into resources
  • More information

Industry News

E-newsletter

Sign up to our free e-newsletter, sent weekly to industry professionals around the world. We'll also let you know each time a new issue of PM Review magazine is available.

Subscribe for a FREE digital magazine

PM Review is the leading international magazine for the Powder Metallurgy industry.
Published four times a year, it is available as a free download or through a print subscription

Connect with us

Powder Metallurgy: The original net-shape production process

Powder Metallurgy components are relied upon by a wide variety of manufacturing industries, from automotive to power tools, household appliances, chemical engineering, filtration and more.

The main reason for the technology’s success is its cost-effectiveness at producing high volumes of net-shape components, combined with its ability to allow the manufacture of products that, because of the production processes, simply cannot be manufactured by other methods.

To discover more about how the technology has revolutionised component production, browse our Introduction to Powder Metallurgy.

Latest industry news

Copy link
Powered by Social Snap