Researchers at the University of Pennsylvania, USA, have developed a process that could enable efficient recycling of the rare earth metals, neodymium and dysprosium. These elements are used in the manufacture of small, powerful magnets that are found in many high-tech devices.

Before-Seperation--

Starting with the two elements as a mixed powder,

a metal-binding molecule known as a ligand is applied.

In contrast to the energy-intensive industrial process currently used to separate rare earths, the University of Pennsylvania’s method is claimed to work almost instantaneously at room temperature and uses standard laboratory equipment. Sourcing neodymium and dysprosium from used electronics rather than the ground would increase their supply at a fraction of the financial, human and environment cost.

The research, published in Angewandte Chemie International Edition, was led by Eric J. Schelter, Assistant Professor in the Department of Chemistry in Penn’s School of Arts & Sciences, and graduate student Justin Bogart. Connor A. Lippincott, an undergraduate student in the Vagelos Integrated Program in Energy Research, and Patrick J. Carroll, Director of the University of Pennsylvania X-Ray Crystallography Facility, also contributed to the study.

These thermal qualities are achieved by mixing neodymium with other elements, including the rare-earth metal dysprosium, in different ratios. Because those ratios differ based on the application the magnet is being used for, the two metals need to be separated and remixed before they can be reused.

During-Seperation-

Size differences mean that ligand-neodymium complexes

bind with one another, while their dysprosium

counterparts do not

“It’s, in principle, easier to get the neodymium and dysprosium out of technology than it is to go back and mine more of the minerals they are originally found in,” Schelter stated. “Those minerals have five elements to separate, whereas the neodymium magnet in a wind turbine generator only has two.”

Currently, whether purifying the neodymium and dysprosium out of minerals or out of an old power tool motor, the same costly and energy-intensive process is used. The technique, known as liquid-liquid extraction, involves dissolving the composite material and chemically filtering the elements apart. The process is repeated thousands of times to get useful purities of the rare-earth metals, and so it must be conducted on an industrial scale.  

Rather than this liquid-liquid method, Schelter’s team has devised a way to separate the two metals. “When we started,” Bogart stated, “our goal was to make rare earth separations simpler and more efficient and we have made strides towards just that. We have designed a way to separate the two metals by selectively dissolving the neodymium in a solution and leaving behind the dysprosium as a solid. This quick and easy method has allowed us to separate equal mixtures of the metals into samples that are 95% pure.”

After-Seperation-

This binding increases the solubility of the neodymium over

that of the dysprosium, allowing the former

to be filtered off.

Starting with the two elements as a mixed powder, a metal-binding molecule known as a ligand is applied. The type of ligand the research team designed has three branches, which converge on the metal atoms and hold them in the aperture between their tips. Because of neodymium’s slightly larger size, the tips don’t get as close together as they do around dysprosium atoms.    

“The difference in size between the two ions is not that significant, which is why this separation problem is difficult,” Schelter said, “But it’s enough to cause that aperture to open up more for neodymium. And, because it is more open, one ligand-neodymium complex can combine with another, and that really changes its solubility.”

The combination of the two neodymium complexes, known as a dimer, encapsulates the neodymium ions, enabling them to dissolve in solvents like benzene or toluene. The dysprosium complexes do not dissolve, enabling the two metals to be easily separated. Once apart, an acid bath can strip the ligand off both metals, enabling it to be recycled as well.

“If you have the right ligand, you can do this separation in five minutes, whereas the liquid-liquid extraction method takes weeks,” continued Schelter. “A potential magnet recycler probably doesn’t have the capital to invest in an entire liquid-liquid separations plant, so having a chemical technology that can instantaneously separate these elements enables smaller scale recyclers to get value out of their materials.”

Future work will involve improving the stability of the ligand so it is less likely to fall off before the metals are separated. “These results are encouraging,” Bogart said. “We feel that through slight adjustments to the system, the purity level could be increased even further.”

Further modification of the ligand could enable other rare earths in technology products, such as compact fluorescent light bulbs, to be recycled this way. The research was supported by the Early Career Research Program of the US Department of Energy’s Office of Science and the Research Corporation for Science Advancement.

http://www.upenn.edu/pennnews/news/penn-research-simplifies-recycling-rare-earth-magnets 

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Powder Metallurgy’s challenge: How does automotive’s reliance on model-based decision making impact our industry?
  • How to make metal powders. Part 4: Centrifugal and other special atomisation methods
  • Precision and energy efficiency in PM press technology: Insights from Ceramitec 2022
  • Historic traditions and new innovations: refractory metals and hard materials at the 20th Plansee Seminar
  • Tailoring a speciality alloy for Additive Manufacturing: From powder production to parameter optimisation
  • Understanding the compaction and sintering effects of four commonly used lubricants in Powder Metallurgy

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

From the industry…

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
Download PDF
Share via
Copy link