Tiangong aiming at 5000 tons annual production of Powder Metallurgy tool steel

News
April 4, 2018

April 4, 2018

China’s Tiangong International Co., Ltd., Jiangsu, is reportedly planning to produce 5,000 tons of Powder Metallurgy tool steels annually, as the domestic market continues to show rapid growth.

According to the Chinese website Steelclik, the annual demand for Powder Metallurgy tool steel in China is around 500 tons, growing at a rate of 30% to 40% per year. Currently, China is said to rely heavily on imports from producers in the US, Japan, Sweden and Russia.

Tiangong’s investment in related equipment will see a first phase production of around 2,000 tons, rising to 5,000 tons per year. Established in 1981, the company manufactures a wide range of high speed steels, die steels and cutting tools.

www.tiangong-tools.com

News
April 4, 2018

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Phoenix Sintered Metals: A story of transformation, growth and community from America’s PM heartland
  • World PM2024 Yokohama: The stage is set for the PM industry to find a path to sustainable growth
  • The state of Europe’s hard magnets industry and the challenge of optimising the mass production of Nd2Fe14B permanent magnets

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link