The Low Gas Consumption continuous furnace: Delivering increased efficiency across PM

June 23, 2021

With over three decades of experience manufacturing furnaces for the Powder Metallurgy industry, India’s Fluidtherm Technology Pvt Ltd saw the need for a furnace with an increased cooling rate and reduced gas consumption.

The company turned to its R&D department to develop a patent-applied Low Gas Consumption (LGC) furnace. The LGC furnace acts as a hybrid between mesh belt and pusher furnaces, utilising the best aspects of each to create an innovative new product.

The motivation behind the development was to increase the capacity of the cooling blower in the sinter hardening unit of mesh belt sintering furnaces, in hope of increasing the cooling rate. This new design concept was also found to reduce gas consumption substantially and made it possible to change the way several thermal processes are performed.

In the Summer 2021 issue of Powder Metallurgy Review (Vol. 10 No. 2), N Gopinath of Fluidtherm Technology, reports on the goals behind the LGC furnace’s development, and what can be achieved using this innovative new furnace concept.

This article, along with the full magazine, is available to read in full online using the embedded browser above or to download as a pdf.

www.pm-review.com

Latest Industry News

Download the latest issue of PM Review

Our latest issue is now available to download in PDF format, free of charge.

As well as an extensive Powder Metallurgy industry news section, this 92-page issue includes the following exclusive articles and reports:

  • The state of Germany’s Powder Metallurgy industry: From the coronavirus pandemic to the EV revolution
  • CM Furnaces: A stalwart of the industrial furnace segment reflects on seventy-five years of thermal processing innovation
  • Liberty Powder Metals: The Liberty Steel spin-out targeting high-quality metal powder production for advanced manufacturing processes
  • The Low Gas Consumption continuous furnace: Delivering increased efficiency across a range of PM applications
  • Eliminating conflict minerals: A new standard for the assurance of conflict-free materials across the supply chain
  • More information

Industry News

E-newsletter

Sign up to our free e-newsletter, sent weekly to industry professionals around the world. We'll also let you know each time a new issue of PM Review magazine is available.

Subscribe for a FREE digital magazine

PM Review is the leading international magazine for the Powder Metallurgy industry.
Published four times a year, it is available as a free download or through a print subscription

Connect with us

Powder Metallurgy: The original net-shape production process

Powder Metallurgy components are relied upon by a wide variety of manufacturing industries, from automotive to power tools, household appliances, chemical engineering, filtration and more.

The main reason for the technology’s success is its cost-effectiveness at producing high volumes of net-shape components, combined with its ability to allow the manufacture of products that, because of the production processes, simply cannot be manufactured by other methods.

To discover more about how the technology has revolutionised component production, browse our Introduction to Powder Metallurgy.

Latest industry news

Copy link