TAT Technologies video offers simplified understanding of sintering for PM

September 11, 2018

TAT Technologies video offers simplified understanding of sintering for PM

TAT Technologies’ new video is designed to offer a simplified understanding of the sintering process (Courtesy TAT Technologies)

 

TAT Technologies has released a video which aims to explain the sintering process used in Powder Metallurgy. Aimed to help viewers visualise the journey taken by a PM part from one end to the other of a typical sintering furnace, the two-minute video shows the physical, mechanical and metallurgical transformations undertaken by Fe-Cu-Carbon-Lube green PM parts in a two-hour sintering cycle.

The video is available to view for free via YouTube and offers a simple visual reference for the internal processes that take place when PM material is sintered cleanly and efficiently. Click here to view now.

TAT Technologies runs a series of popular sintering courses from its training centre in St. Mary’s, Pennsylvania, USA.  The courses, ‘Preparation for Better Sintering’ and ‘Sintering – Ferrous PM’, are aimed at employees in the PM industry who want to learn more about the necessary fundamentals of delubing and sintering.  Both offer hands-on training and have common objectives.

The company has announced that the next dates for its sintering courses will be October 16–19, 2018 (Preparation for Better Sintering), and October 22–25, 2018 (Sintering — Ferrous PM).

www.tat-tech.com

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Burgess-Norton and Amsted Automotive: How a legacy automotive supplier is growing with, not despite, electrification
  • Meeting sustainability demands in PM: High-temperature sintering of nickel- and copper-free powder mixtures for low alloyed PM parts
  • World PM2022: An overview of the status and trends in the global PM industry
  • A novel approach for the production of metal powders with tailored chemical compositions: Amazemet’s rePowder
  • Productivity, flexibility, reliability: SACMI’s new press technologies for the changing PM industry
  • Understanding the thermal properties of metal powders: Characterisation of powders using the Hot Disk technique
  • World PM2022: Views on the potential of Field Assisted Sintering for advanced materials

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

From the industry…

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
Download PDF
Share via
Copy link