Strongest titanium alloy aims at improving vehicle fuel economy and reducing CO2 emissions

News
June 20, 2016

June 20, 2016

An improved titanium alloy, claimed to be stronger than any commercial titanium alloy currently on the market, is reported to get its strength from the novel way atoms are arranged to form a special nanostructure. For the first time, researchers have been able to see this alignment and then manipulate it to make a low-cost beta-titanium alloy with high strength.

pnnl

Using Atom Probe Tomography, researchers are able to create an “atomic map” of the arrangement of various atoms in this titanium alloy

As noted in a paper published by Nature Communications, the material is an excellent candidate for producing lighter vehicle parts and that this new found understanding may lead to creation of other high strength alloys.

Researchers at the US Department of Energy’s Pacific Northwest National Laboratory (PNNL), Richland, Washington, knew the titanium alloy made from a low-cost process they had previously pioneered had very good mechanical properties, but they wanted to know how to make it even stronger. Using powerful electron microscopes and a unique atom probe imaging approach they were able to peer deep inside the alloy’s nanostructure to see what was happening. Once they understood the nanostructure, they were able to create the titanium alloy.

At 45% the weight of low carbon steel, titanium is a lightweight but not super strong element. It is typically blended with other metals to make it stronger. Fifty years ago, metallurgists tried blending it with inexpensive iron, along with vanadium and aluminium. The resulting alloy, called Ti185 was very strong, but only in places. The mixture tended to clump, just like any recipe can. Iron clustered in certain areas creating defects known as beta flecks in the material, making it difficult to commercially produce this alloy reliably.

About six years ago, PNNL and its collaborators found a way around that problem and also developed a low-cost process to produce the material at an industrial scale, which had not been done before. Instead of starting with molten titanium, the team substituted titanium hydride powder. By using this feedstock, they reduced the processing time by half and they drastically reduced the energy requirements, resulting in a low-cost process in use now by a company called Advance Materials Inc. ADMA co-developed the process with PNNL metallurgist Curt Lavender and sells the titanium hydride powder and other advanced materials to the aerospace industry and others.

Researchers knew that they could make this alloy even stronger by heat-treating it. Heating the alloy in a furnace at different temperatures and then plunging it into cold water essentially rearranges the elements at the atomic level in different ways thereby making the resulting material stronger. The PNNL team knew if they could see the microstructure at the nano-scale they could optimise the heat-treating process to tailor the nanostructure and achieve very high strength.

“We found that if you heat treat it first with a higher temperature before a low temperature heat treatment step, you could create a titanium alloy 10-15% stronger than any commercial titanium alloy currently on the market and that it has roughly double the strength of steel,” stated Arun Devaraj a material scientist at PNNL. “This alloy is still more expensive than steel but with its strength-to-cost ratio, it becomes much more affordable with greater potential for lightweight automotive applications,” added Vineet Joshi a metallurgist at PNNL.

Devaraj and the team used electron microscopy to zoom in to the alloy at the hundreds of nanometers scale, about 1,000th the width of an average human hair. Then they zoomed in even further to see how the individual atoms are arranged in 3-D using an atom probe tomography system at EMSL, the Environmental Molecular Sciences Laboratory, a DOE Office of Science User Facility located at PNNL.

The atom probe dislodges just one atom at a time and sends it to a detector. Lighter atoms “fly” to the detector faster, while heavier items arrive later. Each atom type is identified depending on the time each atom takes to reach the detector and each atom’s position is identified by the detector. Thus scientists are able to construct an atomic map of the sample to see where each individual atom is located within the sample.

By using such extensive microscopy methods, researchers discovered that by the optimised heat treating process, they created micron sized and nanosized precipitate regions, known as the alpha phase in a matrix called the beta phase, each with high concentrations of certain elements.

“The aluminium and titanium atoms liked to be inside the nano-sized alpha phase precipitates, whereas vanadium and iron preferred to move to the beta matrix phase,” said Devaraj. The atoms are arranged differently in these two areas. Treating the regions at higher temperature of a 1,450 degrees Fahrenheit achieved a unique hierarchical nano structure.

When the strength was measured by pulling or applying tension and stretching it until it failed, the treated material achieved a 10-15% increase in strength which is significant, especially considering the low cost of the production process.

ti-185

Comparison of tensile strength and strain to failure (elongation) of Ti185 alloy with other commercially available Titanium alloys. The graph in is plotted using CES Selector software, Granta Design, Cambridge, UK. (Image from paper: ‘A low-cost hierarchical nanostructured beta-titanium alloy with high strength’, A Devaraj et al, Nature Communications)

If you take the force you are pulling with and divide it by the area of the material you get a measure of tensile strength in megapascals. Steel used to produce vehicles has a tensile strength of 800-900 megapascals, whereas the 10-15% increase achieved at PNNL puts Ti185 at nearly 1,700 megapascals, or roughly double the strength of automotive steel while being almost half as light.

The team collaborated with Ankit Srivastava, an assistant professor at Texas A&M’s material science and engineering department to develop a simple mathematical model for explaining how the hierarchical nanostructure can result in the exceptionally high strength. The model when compared with the microscopy results and processing led to the discovery of this strongest titanium alloy ever made.

“This pushes the boundary of what we can do with titanium alloys,” added Devaraj. “Now that we understand what’s happening and why this alloy has such high strength, researchers believe they may be able to modify other alloys by intentionally creating microstructures that look like the ones in Ti185.”

For instance, aluminium is a less expensive metal and if the nanostructure of aluminium alloys can be seen and hierarchically arranged in a similar manner, that would also help the auto industry build lighter vehicles that use less fuel and put out less carbon dioxide that contributes to climate warming.

www.pnnl.gov

 

News
June 20, 2016

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • “Scrap is the new gold” and other hardmetal and hard materials insights from Euro PM2023 Congress, Lisbon
  • IperionX: A Powder Metallurgy route to lower-cost recycled titanium plate, billet, bar and preforms with reduced CO2 emissions
  • A review of the sintering of iron-copper-carbon alloys for structural Powder Metallurgy applications

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link