Sintex a/s, headquartered in Hobro, Denmark, recently presented its new corrosion-resistant PM duplex stainless steel component at the Stainless Steel World Duplex in Rotterdam, the Netherlands.

Sintex has stated that its duplex stainless steels are suitable for use within severe environments and can be processed via Metal Injection Moulding, Binder Jetting and Material Extrusion. The company supplies to a wide variety of industries across the world, including energy, automotive, medical, electronics.

At the Stainless Steel World Duplex conference, Peter Kjeldsteen, Chief of Marketing & Innovation, gave an introduction to the company’s duplex stainless steels, discussing its applicability and future potential. The company also covered the corrosion resistance and mechanical properties, the possibility of reducing the need for welded and bolted assemblies, and whether complex geometries are needed in stainless steels.

www.sintex.com

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Phoenix Sintered Metals: A story of transformation, growth and community from America’s PM heartland
  • World PM2024 Yokohama: The stage is set for the PM industry to find a path to sustainable growth
  • The state of Europe’s hard magnets industry and the challenge of optimising the mass production of Nd2Fe14B permanent magnets

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link