Increasing density and reducing lubricant content with AncorMax 225 from Hoeganaes Corporation
February 26, 2014
As the applications for Powder Metallurgy (PM) structural parts become increasingly more demanding there is a need for parts with higher strength, hardness, and ductility. The most effective way to ... Read more »