Nanocrystalline powder metallurgy alloys offer lighter and harder alternative to aluminum and steel
September 3, 2010
Powdermet Inc., Ohio, USA has announced the development of a new powder metallurgy (PM) approach to the production of bulk nanocrystalline metallic composites. Working with the Army Research Laboratory and Case Western Reserve University, Powdermet recent ... Read more »