Polymet launches new thermal spray powder product line

News
August 20, 2012

August 20, 2012

Polymet Corporation has announced the introduction of High Velocity Oxy-Fuel (HVOF) powders to compliment its thermal spray product line.

Prior to the addition of powder to the product line, Polymet provided thermal spray materials for wire arc spray and wire flame spray processes. Now, tungsten carbide-based powders for HVOF systems will be available.

Tungsten carbides have excellent wear resistance and corrosion resistance properties and the company will focus on the WC-12Co, WC-17Co, WC-10Ni, and WC-10Co-4Cr tungsten carbides. Each product will be -45/+15 microns in size.

“Through this new product offering, Polymet will be reaching new prospects and finally meeting the needs of existing customers requiring powder in addition to wire,” stated Pete Humphries, Marketing Manager for Polymet.

For more information contact: [email protected]

www.polymet.us 

 

Posted by: Paul Whittaker, Editor ipmd.net, [email protected]   

News | Articles | Market reviews | Search directory | Subscribe to e-newsletter

News
August 20, 2012

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Phoenix Sintered Metals: A story of transformation, growth and community from America’s PM heartland
  • World PM2024 Yokohama: The stage is set for the PM industry to find a path to sustainable growth
  • The state of Europe’s hard magnets industry and the challenge of optimising the mass production of Nd2Fe14B permanent magnets

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link