Linde LLC, located in Bridgewater, New Jersey, USA, a member of The Linde Group, has introduced Hydroflex, an advanced atmosphere control system that allows clean and bright oxide-free annealing of steel, stainless steel, copper, bronze or brass. The system can also be used in sintering and brazing applications.

“The Hydroflex advanced atmosphere control can use one or more carrier gases – nitrogen or argon – to maintain the furnace pressure while a controlled ratio of hydrogen helps prevent oxidation,” explains Akin Malas, Head of Application Technology, Metals & Glass Market, Linde LLC.

“Uses go beyond annealing,” added Grzegorz Moroz, Program Manager, Heat Treatment and Atmospheres, Linde LLC. “The Hydroflex control system can help optimise your process efficiency and enhance productivity of your process regardless of whether you are annealing, sintering or brazing copper, steel, stainless steel, bronze or brass,”

“First, it contributes to repeatable parts quality. In addition, a bright oxide-free finish means less rework, and a high reliability process means higher productivity,” added Moroz.

Linde offers a variety of advanced gas control technologies and engineering services for heat treatment furnaces. In addition, engineers at Linde Application Technology Centers can develop new gas supply systems for heat treatment processes and improve the control systems of existing processes. Metallography laboratory services include material analyses, scanning electron micrography (SEM) and a variety of hardness tests.

www.lindeus.com

News
August 25, 2016

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • “Scrap is the new gold” and other hardmetal and hard materials insights from Euro PM2023 Congress, Lisbon
  • IperionX: A Powder Metallurgy route to lower-cost recycled titanium plate, billet, bar and preforms with reduced CO2 emissions
  • A review of the sintering of iron-copper-carbon alloys for structural Powder Metallurgy applications

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link