In this article, the fourth of our reports from the PM2010 World Powder Metallurgy Congress in Florence, Italy, Dr Georg Schlieper reports on notable developments in the hard materials industry.

Fatigue testing of hardmetals re-invented

The European Hard Materials Group (EHMG), a special interest group within the European Powder Metallurgy Association (EPMA), is composed of the leading European manufacturing and research organisations in the hard materials sector.

The group has initiated a feasibility study for an innovative high cycle fatigue test of hard materials at a high frequency of 20 kHz. The results of this study were presented by Prof Herbert Danninger of the Technical University of Vienna, Austria, who had also been in charge of the research, at an Open Meeting of the EHMG in Florence, Italy. 

Fatigue testing is a time consuming and costly task, and a high number of load cycles must be applied under alternating loading conditions to determine service life. It is easy to see that the frequency of alternating loading determines the time required to apply a certain number of load cycles. A high load frequency can, therefore, substantially reduce the time and costs of fatigue testing.

g_fig_1

Fig. 1 shows a schematic of the test rig used. The alternating load was generated by an ultrasonic transducer, with an acoustic horn transferring the vibration to a coupling piece attached to the test specimen. The other end of the specimen was free. The loading mode in this test was tension-compression and a splash cooling unit was installed around the test specimen in order to prevent the sample from heating up. A photograph of the actual test rig is shown in Fig. 2.

g_fig_2 

The aim of the feasibility study was to qualify the test for hard materials and define the geometry and preparation route of test specimens (Fig. 3). Of particular importance is the total length of the sample which must match with the test frequency in order to ensure optimum resonance. A total length of 24 mm was proposed with a test diameter at the thinnest point of 4 mm. Depending on the elastic modulus of the tested material the test frequency has to be fine tuned.

g_fig_3The surface finish is also important as fatigue cracks tend to start at the surface. The surface must be free from residual stresses that might bias the results.

The application of high frequency fatigue testing at 20 kHz allowed, for the first time, to extend the number of load cycles into the gigacycle range (10 gigacycles = 10 billion cycles = 1010 cycles). The duration of the 10 gigacycle test was just a few days. At a frequency of 30 Hz, which is common in fatigue testing, it would have taken roughly 10 years.

 

The push-pull mode applied for loading was reported to put a significantly larger part of the sample volume under stress than the bending mode. Therefore it was assumed that the test should be more sensitive to material defects such as residual pores, cobalt pools or excessively large tungsten carbide grains.

An extensive research project is being planned at the Technical University of Vienna where the potential of the new fatigue test will be fully exploited.

Advanced technique to study the cobalt binder phase in hardmetals

Dr Jessica Marshall of Sandvik Hard Materials Research in Coventry, United Kingdom, investigated the binder phase in WC-Co hardmetals using electron backscatter diffraction (EBSD). This is a highly sophisticated metallographic technique which is performed in an electron microscope.

The preparation of test samples begins with grinding and polishing, as in optical metallography. Samples are diamond polished to 0.25 µm prior to 5 minutes 0.05 µm colloidal silica polish, then ion-beam etched for 90 minutes in an argon atmosphere. Finally, samples are etched using Murakami’s reagent.

Samples were mounted in a custom-built holder tilted at 70° to the horizontal, eliminating the need for adhesive. The orientation image mapping technique that was applied reduced the tungsten carbide grains to small grey regions and made the binder phase orientation visible. An example is shown in Fig. 4.

g_fig_4 

The colours in this image represent the orientations of cobalt grains, with each grain depicted by one colour. The size of the cobalt grain was often 300 microns or more whereas the average grain size of tungsten carbide was only 3 microns. The boundaries between cobalt grains often appeared interlocked, which is unusual for metallic microstructures. The author argued that true Co-Co grain boundaries are much less in hardmetal than WC-Co grain boundaries, as WC-Co hard metals consist of a dispersed tungsten carbide phase surrounded by metallic cobalt.

 

News | Articles | Market reviews | Search directory | Subscribe to e-newsletter

November 17, 2010

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • From powder modification to rejuvenation: Fluidised Bed Reactors in metal powder production and Additive Manufacturing
  • Retech: Enabling the atomisation of reactive and refractory alloys at substantially higher levels of productivity and lower cost
  • Sustainability in Powder Metallurgy: Highlights from the 41st Hagen Symposium
  • Innovations from Japan’s Powder Metallurgy industry: award winners highlight novel automotive and healthcare applications

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link