Hoeganaes open premixing and market support facility in China

News
November 22, 2010

November 22, 2010

Hoeganaes Corporation, headquartered in Cinnaminson, USA, has recently opened a new premixing and market support facility in Danyang, Jiangsu Province, China. The facility will support the growing China powder metallurgy market with quick delivery of press-ready premixes as well as warehousing the full portfolio of the company’s products.

HoeganaesNew_China_FacilityDave Kasputis, President of Hoeganaes Corporation and Stefan Magirius, President of GKN China, conducted the official ribbon-cutting to celebrate the opening of the facility.

Invited guests who also spoke at the opening included Zhou Hai Yang, Vice General Manager of NBTM, one of the largest PM companies in China; Ms. Chen Yue, General Secretary of one of China’s larger PM associations, the CMPMA; and William Wang, China Country Manager for Hoeganaes.

The new facility is focused on serving Hoeganaes’s customers throughout China. This will be accomplished by its provision of a high-quality mixing facility, fully-equipped laboratory with technical support and quality assurance services local to the Chinese market. It will offer short lead-time production of press-ready premixes as well as warehousing the full portfolio of Hoeganaes Corporation products.

Dave Kasputis said, “Our China expansion allows us to significantly improve our support for this critical growth market and is consistent with our strategic worldwide expansion plans to provide powder metallurgy solutions for every part of the world.”

Hoeganaes Corporation is a leading producer of ferrous metal powders for the sintered component, chemical, and welding industries, and serves the global powder metallurgy marketplace. 

 

More information  www.hoeganaes.com 

       

 

News | Articles | Market reviews | Search directory | Subscribe to e-newsletter

News
November 22, 2010

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Phoenix Sintered Metals: A story of transformation, growth and community from America’s PM heartland
  • World PM2024 Yokohama: The stage is set for the PM industry to find a path to sustainable growth
  • The state of Europe’s hard magnets industry and the challenge of optimising the mass production of Nd2Fe14B permanent magnets

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link