Granutools to launch its latest high temperature GranuPack analyser virtually

September 25, 2020

Granutools has now adapted its GranuPack instrument to perform packing dynamic measurement from ambient temperature up to 200°C (Courtesy Granutools)

Granutools, Awans, Belgium, a developer of advanced instruments to measure powder behaviour, has announced it will launch its latest high temperature GranuPack analyser in a virtual event on October 5, 2020.

In many industrial applications involving powders, the powders are processed at high temperature, therefore to predict powder behaviour, the characterisation must be done at the same temperature, the company states.

Granutools reports that it has now adapted its GranuPack instrument to perform packing dynamic measurement from ambient temperature up to 200°C.

During the virtual product launch, Granutools will highlight how GranuPack high temperature can be used to improve Additive Manufacturing, food, and pharma processes.

The webinar presentation will take place Monday October at 9AM CET, with a second at 3PM CET.

Further information and registration details are available here.

www.granutools.com

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Burgess-Norton and Amsted Automotive: How a legacy automotive supplier is growing with, not despite, electrification
  • Meeting sustainability demands in PM: High-temperature sintering of nickel- and copper-free powder mixtures for low alloyed PM parts
  • World PM2022: An overview of the status and trends in the global PM industry
  • A novel approach for the production of metal powders with tailored chemical compositions: Amazemet’s rePowder
  • Productivity, flexibility, reliability: SACMI’s new press technologies for the changing PM industry
  • Understanding the thermal properties of metal powders: Characterisation of powders using the Hot Disk technique
  • World PM2022: Views on the potential of Field Assisted Sintering for advanced materials

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

From the industry…

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
Download PDF
Share via
Copy link