Gasbarre expansion to triple size of its St Marys facility

Companies & MarketsNews
November 2, 2022

November 2, 2022

Gasbarre Products Inc is reported to be expanding its facility in St Marys, Pennsylvania, USA, with an investment of some $5.8 million. The company has leased a 14,000 m2 facility in St Marys, which will triple the size of its current location and create sixteen new jobs, while retaining a further 156 employees across four locations statewide. Gasbarre also plans to relocate operations from Plymouth, Michigan, to the expanded facility.

Gasbarre received a funding proposal from the Donor Committee for Enterprise Development (DCED) for a $64,000 Pennsylvania First grant. As part of its expansion project, the company has committed to creating new jobs at its St Marys facility within three years.

“Our investment in the new facility in St Marys provides an opportunity for Gasbarre to continue to grow and flourish where we have manufactured for nearly fifty years,” stated Alex Gasbarre, CEO. “The work ethic and skills provided by past, current, and future Gasbarre team members provide a strong base for this move. We look forward to adding new team members in the coming months when the move process is completed. The people of Elk County and St. Marys will be key to our success.”

www.gasbarre.com

Companies & MarketsNews
November 2, 2022

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Phoenix Sintered Metals: A story of transformation, growth and community from America’s PM heartland
  • World PM2024 Yokohama: The stage is set for the PM industry to find a path to sustainable growth
  • The state of Europe’s hard magnets industry and the challenge of optimising the mass production of Nd2Fe14B permanent magnets

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link