Fritsch launches new laser particle sizer ANALYSETTE 22 NeXT

June 19, 2020

Fritsch has launched the ANALYSETTE 22 NeXT, a new laser particle sizer (Courtesy Fritsch GmbH)

Fritsch GmbH’s Milling and Sizing division, Idar-Oberstein, Germany, has released its new laser particle sizer, ANALYSETTE 22 NeXT which is said to be ideal for particle size analysis in production and quality control, research and development, or for controlling manufacturing processes.

The ANALYSETTE 22 NeXT Micro has a measuring range of 0.05–1500 µm for all typical measurement tasks or the high-end instrument ANALYSETTE 22 NeXT Nano with an extra-wide measuring range of 0.01–3800 µm for maximum precision and sensitivity for smallest particles with an additional detector system.

The company states that the new generation ANALYSETTE 22 NeXT operates like every Fritsch laser particle sizer with the patented reverse fourier design. The laser particle sizer operates with only one laser and is said to not need an additional light source even for backward scattering. It records the entire measuring range with only one scan, making work faster as more measurements can be conducted at the same time, reports Fritsch.

The company explains that with its reduced design and solid engineering, the dispersion unit of the ANALYSETTE 22 NeXT is designed for especially long service life and is practically maintenance-free.A powerful centrifugal pump, with individually adjustable speed ensures stable measuring in the dispersion unit.

www.fritsch.de

In the latest issue of PM Review…

PM Review Spring 2023

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • GKN Powder Metallurgy: A strategic vision for the future of permanent magnets for EVs
  • Building trust in the Powder Metallurgy industry: The role of standardisation and an update on recent work by ISO/TC 119
  • High-volume powder production for Additive Manufacturing: SMS group’s continuous metal powder production process
  • Development of enhanced-performance PM brake pads for high-speed trains by Beijing Tianyishangjia New Material Corp., Ltd.
  • The START project: Creating a sustainable supply chain for green energy harvesting products by Powder Metallurgy
  • World PM2022: Reviewing three innovative methods for metal powder production

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

From the industry…

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
Download PDF
Share via
Copy link