Erasteel takes majority share in Metallied
October 19, 2011
Erasteel has announced it has taken over majority share in the Spanish metal powder supplier, Metallied Powder Solutions S.A.
Metallied, based in Irun, Spain, was created in 2007 and is a spin-off of CEIT based in San Sebastian, Spain, a R&D centre with strong expertise in material science.
Metallied specialises in small batches of tailor made fine powders available in a wide range of alloys thanks to its state-of-the-art and innovative powder atomisation equipment.
Erasteel, a wholly owned subsidiary of Eramet, is the world leading producer of gas-atomised metal powders, such as high speed steels, stainless steels and other specialty alloys for high performance tooling and mechanical component markets, with industrial facilities in Sweden, France, UK as well as in North America and Asia.