EOS releases NickelAlloy HAYNES 282 for M290 and M400-4 machines

July 8, 2022

The microstructure of EOS NickelAlloy Haynes 282 after post-processing using standard solution & standard two-step ageing heat treatment (Courtesy EOS)
The microstructure of EOS NickelAlloy Haynes 282 after post-processing using standard solution & standard two-step ageing heat treatment (Courtesy EOS)

EOS GmbH, headquartered in Krailling, Germany, has introduced EOS NickelAlloy HAYNES® 282®for its EOS M290 and EOS M400-4 Additive Manufacturing machines. The material is a precipitation-strengthened nickel-base superalloy with a combination of high temperature strength, thermal stability and fabricability. Typical applications for the material include aerospace and rocket engine components, turbomachinery and gas turbine parts and energy industry components.

In as-built condition, EOS NickelAlloy HAYNES 282, reputedly has low strength and high ductility. Solution and ageing heat treatments are required to produce the microstructure and strengthening phases for high temperature performance.

EOS has characterised two heat treatment options: (1) recrystallisation solution treatment & standard two-step ageing and (2) standard solution & standard two-step ageing. Heat treatment Option 1 is recommended for properties closest to wrought HAYNES 282.

www.eos.info

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Phoenix Sintered Metals: A story of transformation, growth and community from America’s PM heartland
  • World PM2024 Yokohama: The stage is set for the PM industry to find a path to sustainable growth
  • The state of Europe’s hard magnets industry and the challenge of optimising the mass production of Nd2Fe14B permanent magnets

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link