EOS aluminium alloy powder now from 100% recycled feedstock

March 3, 2025

EOS demonstration bracket additively manufactured on an EOS M 290 using AlSi10Mg (Courtesy EOS)
EOS demonstration bracket additively manufactured on an EOS M 290 using AlSi10Mg (Courtesy EOS)

EOS GmbH, headquarted in Krailling, Germany, has announced that one of its most popular metal powders, EOS Aluminium AlSi10Mg, is now produced with 100% recycled feedstock.

The company reported that increasing the recycled content to 100% has resulted in a 77% CO2e reduction from the prior material, and it now achieves an 83% CO2e reduction compared to AlSi10Mg made from 100% virgin raw material.

THE WORLD OF POWDER METALLURGY TO YOUR INBOX
Subscribe to our weekly newsletter
Sign up

EOS Aluminium AlSi10Mg was first added to EOS’ Responsible Products portfolio in April 2024 when it began incorporating 30% recycled feedstock, achieving a 25% CO2e reduction. While EOS Aluminium AlSi10Mg now employs 100% recycled feedstock, the resulting material maintains the same properties, characteristics and performance in additively manufactured parts, ensuring existing customers do not need to requalify applications.

“We’re proud to have developed our first EOS metal material made with 100% recycled feedstock and to have achieved so much in less than a year. We will continue to explore ways to reduce the carbon footprint of our customers’ applications with every EOS product – from materials and hardware to design optimisation – they all add up to a more responsible end-use product for our customers and the climate,” stated Sophia Heyl, product specialist at EOS.

Björn Hannappel, head of sustainability at EOS, added, “We are continuing our path towards Responsible Manufacturing and expanding our portfolio of Responsible Products stepwise. By minimising waste, reducing the environmental footprint and prioritising eco-friendly materials, organisations can both protect our planet and create a more efficient and resilient business model.”

www.eos.info

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Powder Metallurgy: Discover innovative technologies meeting the demands of vehicle electrification
  • Gevorkyan a.s.: Europe’s fast-growing Powder Metallurgy company achieving success through a diversified customer base
  • Powder Metallurgy in Asia: A status update from the World PM2024 Congress, Yokohama

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link