ECOSINT: The New High Performance Steel Powder

000233Download original article as a PDF

 

000859Italian powder producer POMETON has launched a new high performance steel powder that uses lower amounts of alloying elements, offers excellent hardenability and versatility. This, claims the company, enhances PM part production and reduces overall production costs.

A group of new high strength and cost effective PM steels has been generated by mixing selected combinations of alloying elements (e.g Cr, Mo, Ni, Cu, Mn) in different and predetermined concentrations.

The main purpose was achieving an optimum balance between compressibility, hardenability and properties. The Fe-based powders used served as a basis for preparing blends leading to a range of microstructures after sintering and controlled cooling.

The PM steels presented in this work have a chemical composition within the following limits in wt%: (0.5-2.0)Cr, (0.5-1.5)Mo, (0.4-2.0)Ni, (0.1-0.5)Mn, (0-1.0)Cu, (up to 0.75)C, Fe-balance.

For identification in this work “ECOSINT A” corresponds to a lean material without Cu while materials B and C additionally contain defined concentrations of Ni and Cu for obtaining blends B(= A + xNi), C(= A + xNi + Cu).

With the powder formulation presented here POMETON addresses this issue developing novel PM steels of enhanced hardenability aiming at offering PM parts producers opportunities for obtaining the benefits of sinter hardening while gaining further processing economy through the use of slower and normal cooling rates.

The chemical composition and alloying method of this newly developed Fe based powder have been tailored to render the critical cooling rate, according to the experimentally determined CCT diagrams, as low as 0.45ºC/s.

000858After sintering at 1120ºC and cooling at 0.45ºC/s the microstructure at the geometrical centre of a cylinder weighing 135 grams is fully martensite, thus indicating the important hardenability and depth of hardness corresponding to these PM steels.

A homogeneous microstructure and a constant hardness profile were characteristic of discs and rings.

High temperature sintering allows obtaining materials within the range of the highest tensile strength available for PM steel.

000857High strength combined with attractive ductility is achieved after normal cooling thus emphasising the sinter-hardening characteristics of the developed steels.

 

 

Pometon S.p.A.

Via Circonvallazione, 62

I-30030 Maerne (VE), Italy

Tel: +39 041 290 3611 Fax: +39 041 641 624

www.pometon.com

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • From powder modification to rejuvenation: Fluidised Bed Reactors in metal powder production and Additive Manufacturing
  • Retech: Enabling the atomisation of reactive and refractory alloys at substantially higher levels of productivity and lower cost
  • Sustainability in Powder Metallurgy: Highlights from the 41st Hagen Symposium
  • Innovations from Japan’s Powder Metallurgy industry: award winners highlight novel automotive and healthcare applications

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link