Deutsche Edelstahlwerke offers metal powders for Additive Manufacturing

July 6, 2022

Deutsche Edelstahlwerke offers over 200 grades of powder suitable for Additive Manufacturing (Courtesy Deutsche Edelstahlwerke)
Deutsche Edelstahlwerke offers over 200 grades of powder suitable for Additive Manufacturing (Courtesy Deutsche Edelstahlwerke)

Deutsche Edelstahlwerke, Witten, Germany, now offers a range of gas atomised metal powders for Laser Beam Powder Bed Fusion (PBF-LB) Additive Manufacturing under the brand name Printdur. Available powders include Fe-, Ni- and Co-base metal powders, said to be ideally adapted for the PBF-LB process.

Deutsche Edelstahlwerke has more than 160 years of experience in steel production, and draws on this knowledge to provide support to its customers in determining the parameters necessary for their powders, and testing completed powders to customer specifications using its in-house PBF-LB AM capabilities.

Currently, the company produces over 200 metal powder alloys.

www.dew-stahl.com

Deutsche Edelstahlwerke offers over 200 grades of powder suitable for Additive Manufacturing (Courtesy Deutsche Edelstahlwerke)

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Hot Isostatic Pressing for the production of large, near-net shape components
  • Safeguarding PM part usage in a new automotive industry
  • How to make metal powders., Part 3
  • Company profile: Jiangxi Yuean Advanced Materials

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

From the industry…

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
Download PDF
Share via
Copy link