Constellium launches Aheadd® high-performance aluminium powders

June 23, 2020

Poly-Shape additively manufactured these functional hydraulic blocks using Constellium’s Aheadd® alloy (Courtesy P. Urvoy/Poly-Shape)

Constellium, a global  manufacturer of high value-added aluminium products, headquartered in Paris, France, has launched Aheadd®, its new aluminium powder aimed at the Additive Manufacturing sector.

The the new powder is said to be tailored  to customer needs for a wide range of applications including aerospace, motorsports and defence industries. The company stated that the Aheadd powder brings unmatched thermal stability, allowing replacement of titanium in selected applications to reduce weight and cost.

Constellium has signed a contract with Poly-Shape, an AddUp company, , for the development and production of additively manufactured components based on the new Constellium powders.

“As a global leader in innovative aluminium products and solutions, we are at the forefront of the evolving and fast-changing Additive Manufacturing market, and we are proud to be expanding our portfolio to serve and meet the needs of our customers across all industries,” stated Jean-Marc Germain, CEO of Constellium.

“The global Additive Manufacturing market has great potential with new design and production possibilities, and we look forward to further expanding its potential by providing unique and high-performance aluminium powders customised for our customers,” added Germain.

www.constellium.com

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • “Scrap is the new gold” and other hardmetal and hard materials insights from Euro PM2023 Congress, Lisbon
  • IperionX: A Powder Metallurgy route to lower-cost recycled titanium plate, billet, bar and preforms with reduced CO2 emissions
  • A review of the sintering of iron-copper-carbon alloys for structural Powder Metallurgy applications

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link