Gränges launches low CTE aluminium alloy powder for aerospace and automotive applications
April 12, 2022
Gränges Powder Metallurgy, headquartered in Stockholm, Sweden, has launched its first aluminium alloy for Laser Beam Powder Bed Fusion (PBF-LB) Additive Manufacturing, the S220 AM from its DISPAL ... Read more »