Team from ORNL and NETL develop alloy for Additive Manufacturing crack-free, lightweight turbine blades
October 16, 2024
Researchers at Oak Ridge National Laboratory (ORNL), Tennessee, USA, and the US National Energy Technology Laboratory (NETL), have developed and additively manufactured a light, crack-free alloy ... Read more »