Rolls-Royce recycles RAF Tornado parts into additively manufactured jet engine components
February 6, 2025
The UK’s Rolls-Royce has reported its involvement in the ‘Tornado 2 Tempest’ programme, a recycling initiative that is turning old Royal Air Force Tornado components into metal powder. The powder is then used ... Read more »