Aubert & Duval invests €75 million in new SMS closed-die press
January 16, 2024
Aubert & Duval has signed an agreement with SMS Group to purchase a new 6,000 ton hydraulic press, in a deal worth a total of €75 million. To be installed at the company’s Pamiers site in Ariège, France ... Read more »