H.C.Starck introduces new hardmetal binder

November 9, 2007

H.C. Starck, of Goslar, Germany, has introduced a new hardmetal (cemented carbide) binder material designated AMPERSINT® MAP which is based on iron and is said to be a cheaper alternative to the cobalt binder normally used. The company states that in add ... Read more »

Recent issue of Powder Metallurgy review - your go-to resource to stay updated on the world of powder metallurgy and metal powders

OMG sells nickel business to Norilsk

October 29, 2007

OM Group, the Cleveland, Ohio, based producer of cobalt powder and specialist nickel powders, has completed the previously announced sale of its nickel business to Norilsk Nickel for $408 million in cash. Norilsk is Russia’s largest mining and metallurg ... Read more »

Recent issue of Powder Metallurgy review - your go-to resource to stay updated on the world of powder metallurgy and metal powders

QinetiQ adds alloy powders to its nano range

October 20, 2007

QinetiQ Nanomaterials Ltd (QNL) is to commission a new small scale production plant in Farnborough, UK, in October 2007 for its range of nanopowders produced by the plasma vaporisation process – the so-called Tesima® process. ‘The new rig will enable Q ... Read more »

Recent issue of Powder Metallurgy review - your go-to resource to stay updated on the world of powder metallurgy and metal powders

DuPont develops new lower-cost process for titanium powder

October 9, 2007

DuPont Titanium Technologies, based in Wilmington, Delaware, said to be the world’s largest producer of titanium dioxide (TiO2) – a white pigment used widely in the coatings, plastics and paper industries, has developed a new process for making high-pur ... Read more »

Recent issue of Powder Metallurgy review - your go-to resource to stay updated on the world of powder metallurgy and metal powders

GKN’s PM and PIM operations report strong performances

September 20, 2007

GKN PLC reported that its powder metallurgy (PM) business, which includes metal injection moulding (MIM) operations at the Bad Langensalza plant in Germany, reports positive progress during the first six months of 2007 with higher sales, profits, and ... Read more »

Recent issue of Powder Metallurgy review - your go-to resource to stay updated on the world of powder metallurgy and metal powders

In the latest issue of PM Review…

PM Review Spring 2023

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • GKN Powder Metallurgy: A strategic vision for the future of permanent magnets for EVs
  • Building trust in the Powder Metallurgy industry: The role of standardisation and an update on recent work by ISO/TC 119
  • High-volume powder production for Additive Manufacturing: SMS group’s continuous metal powder production process
  • Development of enhanced-performance PM brake pads for high-speed trains by Beijing Tianyishangjia New Material Corp., Ltd.
  • The START project: Creating a sustainable supply chain for green energy harvesting products by Powder Metallurgy
  • World PM2022: Reviewing three innovative methods for metal powder production

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

From the industry…

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
Download PDF