Aubert & Duval creates superalloy heat treatment line

July 27, 2021

With the support of the France Relance recovery plan and The French Agency for Ecological Transition (ADEME), Aubert & Duval, Paris, has announced a new heat treatment line at its facility in Pamiers, France.

The special processes employed in heat treatment are a key area of knowledge for Aubert & Duval, enabling the modification of materials’ and parts’ microstructures to achieve the highest specifications required by its customers, including those in demanding industries such as aeronautics, energy and defence.

Almost all the parts produced by Aubert & Duval’s new Pamiers line undergo heat treatment procedures. As these are post-processing operations, the performance must be right first time in order to not negatively impact lead times or costs.

The new line has been designed to the highest standards in order to reduce safety risks, ensure process & quality control the digitisation, increase productivity & flexibility and make processing greener (an 8% reduction in CO2 emissions was resultant across the entire site).

www.aubertduval.com

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • From powder modification to rejuvenation: Fluidised Bed Reactors in metal powder production and Additive Manufacturing
  • Retech: Enabling the atomisation of reactive and refractory alloys at substantially higher levels of productivity and lower cost
  • Sustainability in Powder Metallurgy: Highlights from the 41st Hagen Symposium
  • Innovations from Japan’s Powder Metallurgy industry: award winners highlight novel automotive and healthcare applications

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link