Randall M German and Animesh Bose’s new book on Binder and Polymer Assisted Powder Processing has been published by ASM International (Courtesy ASM International)

ASM International has published a new book, Binder and Polymer Assisted Powder Processing, co-authored by Randall M German and Animesh Bose.

The 273-page book focuses on the basic principles and options available for the application of polymers and natural organics to powder processing. It links materials, powder characteristics, forming processes and product attributes together to give what the authors believe to be the first unified treatment on polymer-assisted powder processing.

The processes discussed include injection moulding, sinter-based Additive Manufacturing, uniaxial die compaction, tape casting, extrusion, slip casting and slurry casting. In each process, the technical requirements are outlined and polymer candidates are identified.

ASM International explains that the book bridges the practical aspects of cost, availability and safety with fundamental structure, properties, processing and tests. Each chapter concludes with a review of current industrial standards and examples of practices.

The book covers the following topics as dedicated chapters:

  • Engineering powders
  • Binder constituents
  • Binder formulation
  • Powder-binder feedstock mixing and testing
  • Shaping processes
  • Binder removal
  • Sintering densification
  • Component mechanical properties
  • Case studies of powder-binding processing practices
  • Opportunities for powder-binder forming technologies

The book is available to purchase via the company’s website.

www.asminternational.org

Recent issue of Powder Metallurgy review - your go-to resource to stay updated on the world of powder metallurgy and metal powders

In the latest issue of PM Review…

PM Review Spring 2023

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • GKN Powder Metallurgy: A strategic vision for the future of permanent magnets for EVs
  • Building trust in the Powder Metallurgy industry: The role of standardisation and an update on recent work by ISO/TC 119
  • High-volume powder production for Additive Manufacturing: SMS group’s continuous metal powder production process
  • Development of enhanced-performance PM brake pads for high-speed trains by Beijing Tianyishangjia New Material Corp., Ltd.
  • The START project: Creating a sustainable supply chain for green energy harvesting products by Powder Metallurgy
  • World PM2022: Reviewing three innovative methods for metal powder production

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

From the industry…

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
Download PDF
Share via
Copy link