Anhui Yingliu Group installs Quintus Hot Isostatic Press

December 21, 2015

Jan Söderström, CEO of Quintus Technologies (formerly Avure Technologies), joined Frank Du, President of China’s Yingliu Group, to celebrate the inauguration of a Quintus® Hot Isostatic Press (HIP) at the Anhui Yingliu Group Huoshan Casting Co. Ltd. foundry in Anhui province, China, in early December 2015.

quintus

The new HIP is world’s largest in its pressure and temperature class. The new press, model QIH 1.6 x 2.5 – 2000 – 1400M URC, brings several advanced capabilities that enable the Huoshan facility to manufacture products meeting mission-critical performance standards in the aerospace and nuclear power environments.

Operating at a pressure of 200 MPA and temperatures up to 1400°C, the Quintus HIP produces complex components with improved fatigue strength and extended service life, ever-more-important characteristics that are difficult to achieve in traditional manufacturing technology.

“Quintus HIP systems produce parts with excellent isotropic material properties and offer the highest possible density of all available compaction methods,” stated Jan Söderström, CEO of Quintus Technologies.

The event was attended by more than 500 guests, including representatives from prominent Chinese companies in the aviation and nuclear power industries.

www.quintustechnologies.com  

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Burgess-Norton and Amsted Automotive: How a legacy automotive supplier is growing with, not despite, electrification
  • Meeting sustainability demands in PM: High-temperature sintering of nickel- and copper-free powder mixtures for low alloyed PM parts
  • World PM2022: An overview of the status and trends in the global PM industry
  • A novel approach for the production of metal powders with tailored chemical compositions: Amazemet’s rePowder
  • Productivity, flexibility, reliability: SACMI’s new press technologies for the changing PM industry
  • Understanding the thermal properties of metal powders: Characterisation of powders using the Hot Disk technique
  • World PM2022: Views on the potential of Field Assisted Sintering for advanced materials

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

From the industry…

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
Download PDF
Share via
Copy link