Ampal expands US aluminium powder production with new powder line scheduled for mid-2025

MaterialsNews
December 4, 2024

December 4, 2024

United States Metal Powders will add a new aluminium powder manufacturing line at its Ampal facility in Pennsylvania (Courtesy United States Metal Powders, Inc)
United States Metal Powders will add a new aluminium powder manufacturing line at its Ampal facility in Pennsylvania (Courtesy United States Metal Powders, Inc)

United States Metal Powders, Inc (USMP) has announced a new aluminium powder manufacturing line at its Ampal Inc subsidiary based in Palmerton, Pennsylvania, USA. Scheduled to start full production in the summer of 2025, the new line is expected to offer the capability for both nodular and spherical aluminium powder production.

USMP, founded in 1918, is a leading provider of aluminium powders with two production companies, Ampal Inc and Poudres Hermillon, based in La Tour-en-Maurienne, France. Ampal, reported to be the largest producer of aluminium powder in North America, moved its production facility from Flemington, New Jersey, USA, to its current site in 1982 and has been operating in Palmerton for the last 42 years.

THE WORLD OF POWDER METALLURGY TO YOUR INBOX
Subscribe to our weekly newsletter
Sign up

The company’s products are sold globally to a wide variety of end markets, these include the aerospace, defence, chemical, automotive, general industrial, consumer, construction, and energy sectors.

“We are excited to invest in this new capacity in the USA,” stated Eric Degenfelder, President of USMP. “We are committed to the highest level of customer focus and partnership. Our new production line is designed with state-of-the-art technology for safety, productivity and quality. This expansion both supports our growth ambitions and enhances our hallmark certainty of supply through production redundancy. We are continuing to hire new team members in all functions as we grow the company.”

usmetalpowders.com

Download PM Review magazine
MaterialsNews
December 4, 2024

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Powder Metallurgy: Discover innovative technologies meeting the demands of vehicle electrification
  • Gevorkyan a.s.: Europe’s fast-growing Powder Metallurgy company achieving success through a diversified customer base
  • Powder Metallurgy in Asia: A status update from the World PM2024 Congress, Yokohama

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link