Ametek SMP launches new High Green Strength Stainless Steel Powders for Powder Metallurgy

MaterialsNews
June 20, 2024

June 20, 2024

Ametek Specialty Metal Products (SMP) has announced the launch of its new High Green Strength Stainless Steel Powders (Courtesy Ametek SMP)
Ametek Specialty Metal Products (SMP) has announced the launch of its new High Green Strength Stainless Steel Powders (Courtesy Ametek SMP)

Ametek Specialty Metal Products (SMP), Collegeville, Pennsylvania, USA, has announced the launch of its new ‘High Green Strength Stainless Steel Powders’, suitable for a wide range of automotive and industrial Powder Metallurgy parts.

THE WORLD OF POWDER METALLURGY TO YOUR INBOX
Subscribe to our weekly newsletter
Sign up

The new High Green Strength Powders consistently provide a 50% or greater improvement in green strength in 300 and 400 series stainless steel grades relative to powders mixed with standard EBS wax. This enhancement is said to have minimal impact on sintered density, dimensional change, and other properties.

High GS Lubricants for Press & Sinter – Test Results 409Cb (Courtesy Ametek SMP)
High GS Lubricants for Press & Sinter – Test Results 409Cb (Courtesy Ametek SMP)

Manufactured using advanced water atomisation technology, the High Green Strength Powders are reported to reduce part damage during die ejection and part transfer, leading to more efficient processing and lower manufacturing costs.

www.ametekmetals.com

Download PM Review magazine
MaterialsNews
June 20, 2024

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Phoenix Sintered Metals: A story of transformation, growth and community from America’s PM heartland
  • World PM2024 Yokohama: The stage is set for the PM industry to find a path to sustainable growth
  • The state of Europe’s hard magnets industry and the challenge of optimising the mass production of Nd2Fe14B permanent magnets

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link