6K Additive adds angular titanium and chromium powders

MaterialsNews
September 11, 2024

September 11, 2024

6K Additive, a division of 6K, based in North Andover, Massachusetts, USA, has expanded its metal powder portfolio to include both titanium and chromium angular powders. Angular powders are used in a variety of technologies including Additive Manufacturing, Press & Sinter Powder Metallurgy, Metal Injection Molding, and thermal spray.

The move follows the acquisition of Global Metal Powders in November 2023, enabling 6k Additive to bring additional proprietary metal processing in-house to expand its breadth of sustainable revert streams and recycling capabilities for producing angular chromium and titanium powders.

THE WORLD OF POWDER METALLURGY TO YOUR INBOX
Subscribe to our weekly newsletter
Sign up

The powder range, produced via a sustainable manufacturing process, is reported to be highly pure, with low residual content (such as iron).

“The combination of the acquisition of GMP and our own expertise in sizing and metal upcycling for our spherical powders, allows us to offer a sustainable alternative to what is currently available on the market,” explained Frank Roberts, president of 6K Additive. “For years, customers have asked for angular titanium and chromium powder for applications like thermal spray, welding, and MIM. Adding these products to our portfolio is a natural extension of the powders we currently manufacture. We’re excited to supply our customers with products they’ve been seeking from 6K Additive.”

6K Additive has a powder test process with extensive quality control, including in-house analytical capabilities, micro-CT, gas analysis, ICP, XRD, SEM, and EDS. The company’s production facility is ISO certified and qualified to produce metal powders for high-performance markets such as aerospace, defence, and energy.

www.6kadditive.com

Download PM Review magazine

MaterialsNews
September 11, 2024

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Powder Metallurgy: Discover innovative technologies meeting the demands of vehicle electrification
  • Gevorkyan a.s.: Europe’s fast-growing Powder Metallurgy company achieving success through a diversified customer base
  • Powder Metallurgy in Asia: A status update from the World PM2024 Congress, Yokohama

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link